Bonding Performance of a Universal Adhesive to Blood‐ and Blood–Saliva‐Contaminated Mineral Trioxide Aggregate: Effect of Cleaning Methods
Fereshteh Shafiei, Mahtab Memarpour, Samaneh Sarrafi, Zahra Fattah
Key points
From the paper's conclusion- Objectives To evaluate the effect of blood and blood‐saliva contamination on the shear bond strength (SBS) of All‐Bond Universal adhesive to Mineral Trioxide Aggregate (MTA) and to compare the effectiveness of different cleaning protocols in restoring SBS.
Abstract
Objectives To evaluate the effect of blood and blood‐saliva contamination on the shear bond strength (SBS) of All‐Bond Universal adhesive to Mineral Trioxide Aggregate (MTA) and to compare the effectiveness of different cleaning protocols in restoring SBS. Materials and Methods A total of 132 cylindrical MTA‐Angelus specimens were fabricated, allowed to set for 72 h, acid‐etched for 5 s, and randomly divided into 11 groups ( n = 12). G1 served as the uncontaminated control. Groups G2–G11 comprised two contamination conditions (blood and blood–saliva) and five treatment protocols (no treatment, rinsing, phosphoric acid, gallic acid, and Katana Cleaner). G2–G6 comprised blood‐contaminated specimens subjected to no treatment, rinsing only, rinsing followed by phosphoric acid, rinsing followed by gallic acid, or Katana Cleaner, respectively. G7–G11 comprised blood‐saliva‐contaminated specimens treated using the same protocols in the same order. The specimens were bonded with All‐Bond Universal and everX Flow. SBS was measured. Data were analyzed using Welch's ANOVA and Games–Howell post hoc test (α = 0.05). Fracture modes and surface micromorphology were evaluated. Results All decontamination protocols significantly increased SBS compared with the corresponding untreated contaminated groups (all p < 0.001). Phosphoric acid and gallic acid showed significantly higher SBS values than the rinsing and Katana Cleaner groups in two conditions (all p < 0.001), with no significant difference between the two acids. In both blood and blood‐saliva contamination, SBS after phosphoric acid (9.50 ± 1.49 and 9.10 ± 1.46, respectively) and gallic acid treatment (10.35 ± 1.59 and 9.47 ± 1.72, respectively) was comparable to that of uncontaminated control group (8.67 ± 0.98). Conclusion According to this in vitro finding, gallic acid and phosphoric acid etching with prior water rinsing under blood and blood‐saliva contamination may be an effective approach for achieving high resin–MTA bond strength in contaminated conditions. Katana Cleaner with no prior rinsing exhibited lower effectiveness than acidic agents.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of decontamination strategies on the bond strength of a universal adhesive bonded to hemostatic agent-contaminated dentin.Journal of oral biology and craniofacial research · 2026
- The effect of contamination stage and adhesive strategy on the durability of repair bond strength of blood-saliva contaminated aged composite resin.Odontology · 2026
- MDP-based Cleaner Restores the Bond Strength and Chemical Interaction of a Self-adhesive Resin Cement to Blood-contaminated Zirconia.The journal of adhesive dentistry · 2026
- Effect of decontamination on bond strength of a universal adhesive to saliva-contaminated dentin.European journal of oral sciences · 2026
- Tolerance of universal adhesives to saliva and gingival crevicular fluid contamination of dentin.Dental materials : official publication of the Academy of Dental Materials · 2026
- Effect of n-Butyl Cyanoacrylate Coating on the Microhardness of MM-MTA After Exposure to Moisture and Human Blood.Journal of functional biomaterials · 2026