Influence of dentin depth and hemostatic contamination on microtensile bond strength of a universal adhesive: Effect of phosphoric acid re-etching as a rescue protocol.
Gaurav Patri, Debkant Jena, Prasanti Kumari Pradhan, Pratik Agrawal, Akansha Tilokani, Swadheena Patro
Department of Conservative Dentistry and Endodontics, Kalinga Institute of Dental Sciences (KIDS), KIIT Deemed to be University, Bhubaneswar, 751024, Odisha, India.
Key points
From the paper's conclusion- Dentin depth significantly influences the effectiveness of contamination management strategies. Phosphoric acid re-etching partially restores bond strength in superficial dentin but is ineffective in deep dentin, indicating that contamination management is substrate-dependent.
Abstract
BACKGROUND: This study evaluated the influence of dentin depth and surface treatment on the microtensile bond strength (µTBS) of a universal adhesive to dentin contaminated with an aluminum chloride hemostatic agent, and assessed the effectiveness of phosphoric acid re-etching as a contamination management strategy. MATERIALS AND METHODS: Sixty extracted human third molars were assigned to six groups (n=10) based on dentin depth (superficial or deep) and surface treatment (control, contamination, and contamination followed by phosphoric acid re-etching). A universal adhesive was applied in self-etch mode for control and contamination groups, and in etch-and-rinse mode following the rescue protocol. Composite build-up was performed and specimens were thermocycled (10,000 cycles). µTBS was measured using a universal testing machine. Data were analyzed using two-way ANOVA and Tukey's post hoc test (p<0.05). Failure modes were evaluated using stereomicroscopy and analyzed with Pearson's chi-square test. RESULTS: Superficial dentin demonstrated significantly higher µTBS than deep dentin (p<0.001). Aluminum chloride contamination significantly reduced bond strength in both substrates (p<0.05). Phosphoric acid re-etching significantly improved bond strength in superficial dentin (p<0.05) but did not restore control values. In deep dentin, the rescue protocol did not significantly improve bond strength (p>0.05). A significant interaction between dentin depth and surface treatment was observed (p=0.001). CONCLUSIONS: Dentin depth significantly influences the effectiveness of contamination management strategies. Phosphoric acid re-etching partially restores bond strength in superficial dentin but is ineffective in deep dentin, indicating that contamination management is substrate-dependent.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of decontamination strategies on the bond strength of a universal adhesive bonded to hemostatic agent-contaminated dentin.Journal of oral biology and craniofacial research · 2026
- Effect of decontamination on bond strength of a universal adhesive to saliva-contaminated dentin.European journal of oral sciences · 2026
- Effect of mechanical surface pretreatment, acid conditioning, and adhesive strategy on the repair microtensile bond strength of hydrolytically aged short fiber-reinforced resin composite: an in vitro study.BMC oral health · 2026
- Bonding Performance of a Universal Adhesive to Blood‐ and Blood–Saliva‐Contaminated Mineral Trioxide Aggregate: Effect of Cleaning MethodsClinical and Experimental Dental Research · 2026
- The effect of contamination stage and adhesive strategy on the durability of repair bond strength of blood-saliva contaminated aged composite resin.Odontology · 2026
- Comparison of bond strength in fixed multistrand retainers using universal and conventional adhesives: An in vitro study.Dental research journal · 2026