Defect-Related Fatigue Anisotropy in Laser Powder Bed Fusion Ti–6Al–4V: Role of Sub-β-Transus Annealing and Build Orientation
Franklin Onyeka Ochonogor, Mark Walker
Key points
From the paper's conclusion- The results indicate that defect size, morphology, and orientation relative to the load, rather than tensile properties or density, are the likely cause of the anisotropy.
Abstract
Laser powder bed fusion (LPBF) Ti–6Al–4V shows orientation-dependent fatigue behavior that tensile properties and bulk density do not fully explain. Vertical (VT) and horizontal (HZ) specimens were annealed at 850 °C for 2 h (furnace cooling) and characterized by optical and scanning electron microscopy, X-ray diffraction (XRD) with Rietveld refinement, micro-computed tomography (micro-CT), Vickers hardness, tensile tests, and high-cycle fatigue tests (R = 0.1). The annealed material consisted of α + β (approximately 88–92 vol.% α and 8–12 vol.% β). Tensile properties of the two orientations were similar, with HZ specimens slightly stronger and of similar elongation. Despite a bulk density above 99.9%, micro-CT revealed isolated pores of roughly 60–270 μm. At 600 MPa, VT specimens failed after 6.79 × 104 and 7.36 × 104 cycles, whereas HZ specimens failed after 8.82 × 105 and 1.37 × 106 cycles. Fatigue data at other stress levels are limited, so the orientation effect is demonstrated only at 600 MPa, where two specimens per orientation were tested. The results indicate that defect size, morphology, and orientation relative to the load, rather than tensile properties or density, are the likely cause of the anisotropy. An orientation-sensitive descriptor, F = dmax cos2θ, is proposed as a hypothesis; specimen-resolved defect data exist for only three VT specimens, so it remains to be validated. No as-built control was tested, and conclusions apply to the annealed condition.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Mechanical and Fatigue Properties of a Laser Powder Bed Fusion Ti6Al4V Alloy: A Review.Materials (Basel, Switzerland) · 2026
- On Porosity Analysis of Ti-6Al-4V Thin Struts Made by Laser Powder-Bed Fusion: Effects of Build Orientation, Strut Size and Linear Energy DensityJournal of Manufacturing and Materials Processing · 2026
- Importance of surface defect removal and compressive residual stress introduction in improving fatigue strength of powder bed-fused Ti6Al4V and demonstration of fatigue strength beyond that of hot-rolled Ti6Al4VInternational Journal of Fatigue · 2025
- Corrosion-fatigue of L-PBF Ti-6Al-4V lattice struts: role of geometrical imperfections under simulated physiological conditionsInternational Journal of Fatigue · 2026
- Thermo-Geometric Interpretation of Build Orientation and Strut Size on the Microstructure and Mechanical Behaviour of LPBF-Fabricated Ti–6Al–4V BCC Lattice StructuresMetals · 2026
- The effect of residual stress on the fracture toughness of Ti–6Al–4V produced by laser-based powder bed fusionInternational Journal of Fracture · 2026