The effect of residual stress on the fracture toughness of Ti–6Al–4V produced by laser-based powder bed fusion
D. F. Louw, Melody Neaves, T. H. Becker
Council for Scientific and Industrial Research · Stellenbosch University
Key points
From the paper's conclusion- Apparent fracture toughness ( $${K}_{IC})$$ <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML"> <mml:mrow> <mml:msub> <mml:mi>K</mml:mi> <mml:mrow> <mml:mi>IC</mml:mi> </mml:mrow> </mml:msub> <mml:mrow> <mml:mo>)</mml:mo> </mml:mrow> </mml:mrow> </mml:math> ranged from 25 to 35 MPa m 1/2 , whereas $${K}_{ICeff}$$ <mml:math xmlns:mml="http://www.w3.org/1998/Math/MathML"> <mml:msub> <mml:mi>K<
Abstract
Abstract Laser powder bed fusion (LPBF) imposes steep thermal gradients, resulting in distortion and the formation of significant residual stresses, which often precipitate in-situ cracking at support interfaces and sharp geometric features. To isolate their influence on structural integrity, we combined fracture mechanics testing with residual stress evaluation on as-built compact tension specimens printed in two orthogonal orientations. The experimentally measured apparent stress-intensity factor was deconvolved into mechanical and residual-stress components, yielding a residual-stress-free fracture toughness ( $${K}_{ICeff}$$ K ICeff ). Apparent fracture toughness ( $${K}_{IC})$$ K IC ) ranged from 25 to 35 MPa m 1/2 , whereas $${K}_{ICeff}$$ K ICeff increased to 45–52 MPa m 1/2 . Residual stresses, therefore, depress the material’s residual-stress-free resistance by up to ~ 50% and accentuate orientation-dependent anisotropy. The framework presented offers a route for quantifying process-induced toughness degradation in LPBF alloys.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of process parameters on surface integrity in laser powder bed fusion of Ti-6Al-4V alloyScientific Reports · 2025
- A workflow for residual stress control in laser powder bed fusion manufacturingAdvanced Materials Joining · 2026
- Distortion Behavior of Ti6Al4V and Inconel 718 LPBF Cantilever Specimens: Effects of Scan Strategy and Stress-Relief Heat Treatment.Micromachines · 2026
- Distortion in LPBF Cantilevers Governed by Stiffness-Controlled Stress Redistribution.Materials (Basel, Switzerland) · 2026
- Mechanical and Fatigue Properties of a Laser Powder Bed Fusion Ti6Al4V Alloy: A Review.Materials (Basel, Switzerland) · 2026
- Importance of surface defect removal and compressive residual stress introduction in improving fatigue strength of powder bed-fused Ti6Al4V and demonstration of fatigue strength beyond that of hot-rolled Ti6Al4VInternational Journal of Fatigue · 2025