On Porosity Analysis of Ti-6Al-4V Thin Struts Made by Laser Powder-Bed Fusion: Effects of Build Orientation, Strut Size and Linear Energy Density
Rabiul Islam, Kevin Chou
Key points
From the paper's conclusion- This asymmetry was absent in the 0.25 mm struts, where low pore counts made the metric unreliable.
Abstract
Porosity in laser powder bed fusion (L-PBF) lattice struts remains poorly understood, as the effects of build angle and process parameters are often studied separately. A full factorial design of 27 configurations combined three build angles (40–70°), three strut sizes (0.25–1.25 mm), and three linear energy densities (LED: 0.23–0.35 J/mm). Specimens were fabricated in Ti-6Al-4V on an EOS M270 system and characterized by micro-computed tomography (µ-CT). Statistical analysis showed that all three factors influenced porosity percentage (P%), with a significant size–LED interaction, while only strut size and LED influenced the average volume of individual pores (PVavg), with no significant interactions. P% rose 194% as strut diameter increased from 0.25 to 1.25 mm, climbed steeply between 0.23 and 0.29 J/mm before plateauing, and fell 19% as build angle increased from 40° to 70°. PVavg rose 160% across the LED range and 37% with strut diameter. Spatial segmentation showed that the median down-skin-to-up-skin pore volume ratio in the larger struts fell from 2.0 at 40°, that is, twice the pore volume in the DS region, to 1.3 at 70°. This asymmetry was absent in the 0.25 mm struts, where low pore counts made the metric unreliable.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Beyond Volumetric Energy Density: Process-Window Mapping and Density Metrology for Laser Powder Bed Fusion of High-Strength A20X Aluminium and 304L Stainless SteelJournal of Manufacturing and Materials Processing · 2026
- Role of laser beam shape and energy density in modulating surface quality, porosity, microstructure, and mechanical properties of PBF-LB/M Ti-6Al-4VJournal of Materials Processing Technology · 2026
- Defect-Related Fatigue Anisotropy in Laser Powder Bed Fusion Ti–6Al–4V: Role of Sub-β-Transus Annealing and Build OrientationMetals · 2026
- Effect of Process Co-Factors on Surface Roughness of Subscale Feature Surfaces in Laser PBF of Ti6Al4VJournal of Manufacturing and Materials Processing · 2026
- Effect of process parameters on surface integrity in laser powder bed fusion of Ti-6Al-4V alloyScientific Reports · 2025
- Thermo-Geometric Interpretation of Build Orientation and Strut Size on the Microstructure and Mechanical Behaviour of LPBF-Fabricated Ti–6Al–4V BCC Lattice StructuresMetals · 2026