Comparison of surface integrity, longevity of posterior tooth-colored crowns fabricated by conventional, CAD/CAM, and 3D printing techniques.
Tanner Hunt, Jacob Nichols, Preston Harmon, Neamat Hassan Abubakr
School of Dental Medicine, University of Nevada, Las Vegas, NV, United States. · Biomedical Sciences Department, School of Dental Medicine, University of Nevada, Las Vegas, NV, United States.
Key points
From the paper's conclusion- Within the limitation of the present study material type and fabrication workflow significantly influenced internal and marginal surface roughness of posterior tooth-colored crowns. The crowns survival rates were more closely associated with material type than fabrication method.
Abstract
INTRODUCTION: This in vitro study evaluated internal and marginal surface roughness and simulated thermocycling survival of posterior tooth-colored crowns fabricated using conventional laboratory, CAD/CAM milling, and digital light processing 3D printing workflows. METHODS: The roughness analysis included 46 crowns allocated to six groups: lab-made crowns (n = 6), IPS e.max CAD (n = 8), IPS Empress CAD (n = 8), Lava Ultimate (n = 8), IPS e.max ZirCAD (n = 8), and 3 D SprintRay Ceramic (n = 8). Internal and marginal arithmetic mean roughness (Ra, µm) were measured with a 3D non-contact profilometer. Because residual normality and variance homogeneity assumptions were not satisfied, group differences were analyzed using Kruskal-Wallis tests followed by Holm-adjusted pairwise Mann-Whitney U tests. RESULTS: Internal Ra differed significantly among groups (H = 25.76, df = 5, p < 0.001). 3D printed SprintRay Ceramic showed the highest internal Ra (29.27 ± 5.45 µm) and was significantly rougher internally than every other group after Holm correction. Marginal Ra also differed significantly among groups (H = 41.86, df = 5, p < 0.001). IPS e.max CAD showed the highest marginal Ra (26.81 ± 1.73 µm), followed by lab-made crowns (19.31 ± 6.40 µm), whereas IPS e.max ZirCAD showed the lowest marginal Ra (4.82 ± 1.03 µm). CONCLUSION: Within the limitation of the present study material type and fabrication workflow significantly influenced internal and marginal surface roughness of posterior tooth-colored crowns. The crowns survival rates were more closely associated with material type than fabrication method.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Evaluation of full-veneer crowns fabricated with 3D printing resin material for definitive prostheses: A 1-year randomized controlled prospective study.Journal of dentistry · 2026
- Effects of coffee thermocycling on surface roughness, microhardness, and color stability of permanent crown materialsScientific Reports · 2026
- Influence of post-curing duration on degree of conversion, microhardness, and surface roughness of three commercially available 3D-printed permanent crown resins.Clinical oral investigations · 2026
- Influence of printing orientation, material-printer-workflow system, and glazing on the surface roughness and color stability of 3D-printed resins for permanent crowns.Journal of dentistry · 2026
- Comparison of Implant-Supported Permanent Crowns Produced wıth Different 3D Printed Resins in Terms of Productıon Accuracy, Marginal Fit and Internal Fit: A Comparative in Vitro StudyThe International Journal of Prosthodontics · 2026
- Effect of Finishing Protocols and Simulated Toothbrushing on the Surface Roughness and Color Stability of Conventionally and Digitally Fabricated Interim Restorative MaterialsCoatings · 2026