Department of Prosthodontics, Faculty of Dentistry, Chulalongkorn University, Bangkok, Thailand. · Department of Operative Dentistry, Faculty of Dentistry, Chulalongkorn University, Bangkok, Thailand; Clinic of General-, Special Care-, and Geriatric Dentistry, Center for Dental Medicine, University of Zurich, Zurich, Switzerland.
Key points
From the paper's conclusion- Roughness differed among material-printer-workflow systems, with orientation effects in selected groups. Glazing improved aging-related surface and color stability under the tested conditions. The highest post-aging mean Ra remained below 0.2 µm, but glazed mean ΔE00 values (2.03-2.38) exceeded the acceptability threshold of 1.8.
Abstract
AIM: To evaluate the effects of printing orientation, material-printer-workflow system, and glazing on the surface roughness and color stability of permanent 3D-printed crown resins. MATERIALS AND METHODS: A total of 180 specimens were fabricated using three material-printer-workflow systems (VS, VarseoSmile Crown Plus; SA, Saremco Print Crowntec; CC, Ceramic Crown, SprintRay) with three printing orientations (0°, 45°, and 90°), and two surface conditions (glazed and non-glazed). Specimens were printed, finished, polished, treated (glazed/non-glazed), and subjected to 300 h of artificial accelerated aging. Surface roughness and color stability were measured by atomic force microscopy and spectrophotometry, respectively. Statistical analyses included ANCOVA, ANOVA, and post hoc Bonferroni tests (α = 0.05). RESULTS: Before aging, surface roughness differed among the non-glazed systems at all orientations (all P < 0.05), whereas printing orientation affected only non-glazed SA (P = 0.024). Glazing reduced surface roughness and color change in all material-printer-workflow systems. After aging, printing orientation affected surface roughness in non-glazed SA and CC (both P < 0.001) and glazed VS (P < 0.001), but not color change (all P ≥ 0.05). CC consistently exhibited the highest post-aging surface roughness. CONCLUSIONS: Roughness differed among material-printer-workflow systems, with orientation effects in selected groups. Glazing improved aging-related surface and color stability under the tested conditions. The highest post-aging mean Ra remained below 0.2 µm, but glazed mean ΔE00 values (2.03-2.38) exceeded the acceptability threshold of 1.8. CLINICAL SIGNIFICANCE: The findings inform the selection of material-printer-workflow systems and glazing protocols for 3D-printed restorations. Glazing improved aging-related surface and color stability under the tested laboratory conditions. Post-aging mean Ra remained below the cited 0.2-µm plaque-retention threshold, but glazed mean ΔE00 values were above the acceptability threshold of 1.8.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Different Polishing Systems on the Surface Roughness of 3D-Printed Resins.Materials (Basel, Switzerland) · 2026
- Influence of postprinting cleaning duration and glazing agents on the mechanical and surface properties of three-dimensionally printed dental resins: An in vitro study.The Journal of prosthetic dentistry · 2026
- Effect of modified glaze application protocols on color stability of 3D-printed permanent dental resinsBMC Oral Health · 2026
- Gloss and Surface Roughness of Stained and Polished 3D-Printed Resins Used for the Fabrication of Hybrid Denture Prosthesis: An In Vitro Study.Journal of functional biomaterials · 2026
- Color and Relative Translucency of Three-Dimensionally Printed Restorative Resin Systems: Effects of Build Orientation, Thickness and Staining Conditions.Polymers · 2026
- Influence of post-curing duration on degree of conversion, microhardness, and surface roughness of three commercially available 3D-printed permanent crown resins.Clinical oral investigations · 2026