Modelling and Simulation in Engineering

Quantitative Finite‐Element Evaluation of Field Signature Electrode Configurations for Corrosion Monitoring in Pressurized Pipelines

Yingying Zhang, Yang Li, Shuai Dai, Meng Zhang, You Guo, Lei Liu, Xin Zhang

Key points

From the paper's conclusion
  • These results quantify the trade‐offs among spatial sampling, signal magnitude, monitoring length, and electrode‐system complexity.

Abstract

Electrode configuration strongly influences current homogenization, usable monitoring length, and voltage‐signal level in the Field Signature Method (FSM), but these trade‐offs are often assessed qualitatively. This study establishes a COMSOL‐based finite‐element framework for quantitatively evaluating excitation‐ and measurement‐electrode configurations for corrosion monitoring in a pressurized steel pipe. A stationary Electric Currents model was verified through analytical comparison and mesh‐independence analysis. The relative differences between the finite‐element and analytical results were 0.0124% for the mean axial current density and 0.0109% for the voltage drop over a 1‐m uniform pipe segment. Current uniformity was evaluated using the cross‐sectional coefficient of variation of axial current density, C V J , with a threshold of C V J ≤ 5 % . At a total current of 1 A, the resulting homogenization distances were 135, 68, and 45 mm for one, two, and three excitation‐electrode pairs. Two pairs reduced the adopted homogenization distance from 140 to 70 mm and increased the usable uniform‐current length from 3720 to 3860 mm, whereas the three‐pair configuration provided only a further 40‐mm increase. The current‐density magnitude and electric potential varied approximately linearly with total current. Increasing the excitation‐electrode spacing extended the usable monitoring interval without substantially changing the current‐density magnitude in the uniform‐current region. Increasing the number of radial measurement‐electrode pairs from 2 to 12 reduced the angular sampling interval from 180° to 30°, corresponding to an 83.3% reduction. Reducing the axial measurement‐electrode spacing from 500 to 50 mm decreased the sampling interval by 90%, but also reduced the voltage difference from 23.6715 to 2.4115 μ V, corresponding to 10.2% of the 500‐mm signal. These results quantify the trade‐offs among spatial sampling, signal magnitude, monitoring length, and electrode‐system complexity. The recommendations apply to the investigated geometry, material, and idealized boundary conditions and require further experimental validation.

Read the paper