Corrosion Analysis of Helical Electrodes
Limin Yan, Pengfei Shan, Chunbo Jiang, Rongjuan Sui
Key points
From the paper's conclusion- In this work, the premature corrosion failure of S30408 helical electrodes after 3 months operation was investigated via material characterization and COMSOL simulations.
Abstract
Low‐voltage electrode steam boilers are core pressure‐bearing equipment for clean heating. However, the observed asymmetric corrosion of helical electrodes remains mechanistically unclear, which cannot be explained by existing studies on V‐shaped electrodes in hot water conditions. In this work, the premature corrosion failure of S30408 helical electrodes after 3 months operation was investigated via material characterization and COMSOL simulations. The electrical simulation reveals pronounced geometry‐induced nonuniformity in the calculated current density distribution, with stronger electrical loading on the concave surface and near the electrode edges, where the local value reaches approximately 6.2 × 10 4 A/m 2 . Surface profilometry shows broad, shallow depressions (maximum measured depth approximately 2.1 × 10 2 μm). Flow‐field calculations further show local streamline convergence and recirculation on the concave side, which may reduce liquid renewal and favor retention of steam bubbles generated during boiling. The combined effects of non‐uniform electrical loading and local hydrodynamic conditions provide a plausible explanation for the asymmetric surface attack.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Hierarchical localisation of position of screw metallic internal componentMeasurement Science and Technology · 2026
- Failure Analysis of Acid-Thinned Coiled Tubing Under HTBH Conditions: Role of Inhibitor Depletion and Corrosion Asymmetry.Materials (Basel, Switzerland) · 2026
- Quantitative Finite‐Element Evaluation of Field Signature Electrode Configurations for Corrosion Monitoring in Pressurized PipelinesModelling and Simulation in Engineering · 2026
- Lubrication and Grinding Characteristics of Electrostatically Charged Cutting Fluid AerosolLubricants · 2026
- Rust-Layer Characteristics and Pit Morphology on the Inner and Outer Surfaces of a Retired Q355C Hydropower Penstock.Materials (Basel, Switzerland) · 2026
- Different Plasma Polishing Regimes Induced by Electrolytic FlowJournal of Manufacturing and Materials Processing · 2026