Curing Capacity of Band-Bonding Resinous Adhesives Under 3D-Printed Molar Bands.
Sofia Sideri, Maria Dimitriadi, Nearchos Panayi, Spyridon N Papageorgiou, Theodore Eliades, George Eliades
Department of Biomaterials, School of Dentistry, National and Kapodistrian University of Athens, Athens, Greece. · Faculty of Dentistry, Department of Orthodontics, European University Cyprus, Nicosia, Cyprus.
Key points
From the paper's conclusion- Curing capacity of band adhesives under 3D-printed bands is material-dependent. Blue-shaded OBU and dual-cured BLB showed more uniform conversion, whereas white-shaded TRP exhibited significant depth variations. However, conversion of the adhesives tested under 3D-printed metallic bands was acceptable when a high-intensity light-curing unit was used for an extended irradiation time for orthodontic applications (30 s).
Abstract
AIM: To evaluate the curing efficiency of three resin composite adhesives applied beneath 3D-printed molar bands, by determining their degree of conversion (DC%) at different depths. MATERIALS AND METHODS: Fifteen 3D-printed metallic band specimens were divided into three groups and bonded with Band Lock Blue (BLB), Optiband Ultra Blue (OBU), or Transbond Plus (TRP). Adhesives were applied in 150 μm films and light-cured for 30 s (1200 mW/cm2). Degree of conversion (DC%) was measured at the top, middle, and bottom regions using attenuated total reflection Fourier-transform infrared spectroscopy (ATR-FTIR). Directly irradiated specimens served as controls. Statistical analysis of DC% values was performed with regression modelling at a 5% level. RESULTS: A reduction in conversion beneath the bands compared to non-banded controls was seen, which was dependent on both the adhesive type and the region. For BLB, equally low DC% values were found for banded and non-banded specimens across all regions. Banded OBU specimens had significantly lower DC% compared to non-banded controls at all regions. Finally, TRP banded specimens had significantly lower DC% compared to non-banded controls at the middle and bottom regions, but not at the top region. CONCLUSIONS: Curing capacity of band adhesives under 3D-printed bands is material-dependent. Blue-shaded OBU and dual-cured BLB showed more uniform conversion, whereas white-shaded TRP exhibited significant depth variations. However, conversion of the adhesives tested under 3D-printed metallic bands was acceptable when a high-intensity light-curing unit was used for an extended irradiation time for orthodontic applications (30 s).
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Repair bond strength of composite resin to additively manufactured permanent resin materials: a comparative evaluation of light-cure, self-cure, and dual-cure universal adhesivesBMC Oral Health · 2025
- Marginal and Internal Adaptation Discrepancy and Microtensile Bond Strength of Cemented, Thermocycled 3D-Printed Ceramic-Filled Resin Inlays Processed with Four Post-Curing Protocols: An In Vitro StudyJournal of Composites Science · 2026
- Influence of post-curing duration on degree of conversion, microhardness, and surface roughness of three commercially available 3D-printed permanent crown resins.Clinical oral investigations · 2026
- Effect of different bonding agents and airborne-particle abrasion on shear bond strength and mode of failure between 3D-printed denture tooth-colored specimens and 3D-printed denture bases.BMC oral health · 2026
- 24-Hour Shrinkage Behavior of Ten Resin-Based Composites.Journal of dentistry · 2026
- Light-curing performance of dual-cure and preheated luting materials under simulated restoration thicknesses: an in vitro study.BMC oral health · 2026