Repair bond strength of composite resin to additively manufactured permanent resin materials: a comparative evaluation of light-cure, self-cure, and dual-cure universal adhesives
Esra Yildirim-Manav, Sema Yazici-Akbiyik, Cansu Yikici-Çöl
Lokman Hekim Üniversitesi
Key points
From the paper's conclusion- This study aimed to evaluate the repair bond strength of composite resin to two 3D-printed permanent resin materials using different universal adhesive systems-light-cure, self-cure, and dual-cure-following a standardized air abrasion.
Abstract
BACKGROUND: This study aimed to evaluate the repair bond strength of composite resin to two 3D-printed permanent resin materials using different universal adhesive systems-light-cure, self-cure, and dual-cure-following a standardized air abrasion. METHODS: Seventy-two disc-shaped specimens (n = 12 per group) were fabricated using two different commercial 3D-printed materials: Saremco Crowntec and Bego VarseoSmile Crown Plus. After post-processing, all specimens were thermocycled for 5,000 cycles to simulate aging. The bonding surfaces were then subjected to air abrasion, followed by the application of one of three universal adhesive systems: light-cure (G-Premio Bond), self-cure (Tokuyama Universal Bond II), or dual-cure (Futurabond U). A composite resin (Filtek Z250) cylinder was then bonded and light-cured. Shear bond strength (SBS) was measured, and fracture modes were examined under a stereomicroscope. Data were analyzed using two-way analysis of variance (ANOVA) and Tukey HSD tests (p < 0.05). RESULTS: Self-cure universal adhesives exhibited the highest SBS values, especially in the Bego material group (19.20 ± 2.11 MPa), while the lowest bond strength was observed in the Saremco + light-cure group (14.28 ± 1.23 MPa). Both the adhesive system (p < 0.001) and material type (p = 0.002) significantly affected SBS. Failure mode analysis revealed predominantly adhesive failures in the light-cure groups, and more mixed/cohesive failures in the self-cure and dual-cure groups. CONCLUSIONS: Bond strength of repaired 3D-printed permanent resins is significantly influenced by the adhesive systems and material type. Self-cure universal adhesives provided the most effective bonding performance, particularly when combined with Bego VarseoSmile Crown Plus.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Repair Bond Durability of Selected Thermally Aged CAD/CAM-Milled and 3D-Printed Provisional Restorative Materials Following Different Surface Treatment Protocols: A Comparative In Vitro StudyJournal of Functional Biomaterials · 2026
- In vitro comparison of resin cement bond strength to milled and 3D-printed resins.Journal of the mechanical behavior of biomedical materials · 2026
- Influence of surface pretreatments on the repair bond strength of 3D-printed resin used for permanent restorations: an in vitro study.Frontiers in dental medicine · 2026
- Effect of different bonding agents and airborne-particle abrasion on shear bond strength and mode of failure between 3D-printed denture tooth-colored specimens and 3D-printed denture bases.BMC oral health · 2026
- Evaluation of shear bond strength of 3D-printed flexible denture materials and reline materials.The journal of advanced prosthodontics · 2026
- Marginal and Internal Adaptation Discrepancy and Microtensile Bond Strength of Cemented, Thermocycled 3D-Printed Ceramic-Filled Resin Inlays Processed with Four Post-Curing Protocols: An In Vitro StudyJournal of Composites Science · 2026