Marginal and Internal Adaptation Discrepancy and Microtensile Bond Strength of Cemented, Thermocycled 3D-Printed Ceramic-Filled Resin Inlays Processed with Four Post-Curing Protocols: An In Vitro Study
Hana Fatih Abdulla, Bestoon Mohammed Faraj
Key points
From the paper's conclusion- GP had the numerically lowest discrepancy (77.09 ± 5.48 µm), but its 7.7 µm difference from SP was within measurement uncertainty and not robust to sensitivity analysis.
Abstract
Background: Post-curing may influence the properties of 3D-printed ceramic-filled resin restorations. This study compared four post-curing protocols for adaptation and microtensile bond strength (µTBS) of cemented, thermocycled DLP-printed inlays. Methods: Seventy-six maxillary premolars with standardised MOD cavities received inlays randomised (n = 19) to standard post-curing in air (SP), glycerine-immersed post-curing (GP), or SP plus microwave heating in glycerine (MG; 800 W nominal, 50 s) or autoclaving (AT; 121 °C). After cementation and 5000 thermocycles, adaptation discrepancy—a composite of post-curing change, seating, cement layer and ageing—was measured at 11 points by triple-scan superimposition before µTBS testing of the inlay–cement–dentine complex and failure-mode analysis. Results: Discrepancy (F(3, 37.6) = 24.47, p < 0.001) and µTBS (F(3, 39.8) = 6.09, p = 0.002) differed among protocols. MG showed the largest discrepancy (104.42 ± 13.57 µm; p < 0.01 versus all groups), lower µTBS than GP and SP (15.04 ± 5.13 versus 21.58 ± 4.35 and 20.19 ± 5.33 MPa) and predominantly adhesive failures (68.4% of teeth; interface unidentified). GP had the numerically lowest discrepancy (77.09 ± 5.48 µm), but its 7.7 µm difference from SP was within measurement uncertainty and not robust to sensitivity analysis. AT did not differ from SP. Conclusions: The complete MG protocol was associated with greater discrepancy and lower µTBS; GP did not differ robustly from SP.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effects of Surface Pretreatment Protocols on Interfacial Gap Volume and Shear Bond Strength in the Composite Repair of a Definitive 3D-Printed Dental Resin: An In Vitro Study.Journal of functional biomaterials · 2026
- Repair bond strength of composite resin to additively manufactured permanent resin materials: a comparative evaluation of light-cure, self-cure, and dual-cure universal adhesivesBMC Oral Health · 2025
- Repair Bond Durability of Selected Thermally Aged CAD/CAM-Milled and 3D-Printed Provisional Restorative Materials Following Different Surface Treatment Protocols: A Comparative In Vitro StudyJournal of Functional Biomaterials · 2026
- Effects of nitrogen-assisted post-curing and layer thickness on the properties of a 3D-printed ceramic-reinforced composite resin for permanent crowns under different aging conditions: an in vitro study.BMC oral health · 2026
- Influence of 3D-Printing system on the mechanical and surface properties of a 3D-Printed denture base resin.Journal of applied biomaterials & functional materials · 2026
- Effect of post-polymerization exposure times and material thickness on color stability of 3D-printed definitive restoration resins: An in vitro study.Journal of prosthodontics : official journal of the American College of Prosthodontists · 2026