Key points
From the paper's conclusion- The volume loss ranged from 0.054-0.167 mm³ and the maximum facet depth ranged from 99.6 to 222.7 µm. Significant differences were observed among the resin luting cements and between dual-cure and chemical-cure conditions. However, no significant differences were found between curing conditions within the universal resin luting cements. Additionally, no significant differences were identified between the hand-mixed and auto-mixed versions of the same or similar materials.
Abstract
PURPOSE: To compare the wear resistance of conventional self-adhesive resin luting cements with that of recently developed universal resin luting cements under both dual-cure and chemical-cure conditions, and to evaluate the influence of mixing method (hand-mix or auto-mix). METHODS: Five resin luting cements were evaluated: three universal cements [G-Cem One EM (GUA) and RelyX Universal (RUA) auto-mix types, and G-Cem One neo (GUH) hand-mix type) and two conventional self-adhesive cements (Clearfil SA Luting Multi in hand-mix (SH) and auto-mix (SA) forms, and RelyX Unicem 2 (RA) auto-mix type]. Wear resistance was assessed using an Alabama wear-testing machine. Volume loss (mm³) and maximum facet depth (µm) were measured after wear testing. Statistical analyses were performed to compare differences among materials, curing modes, and mixing methods. RESULTS: The volume loss ranged from 0.054-0.167 mm³ and the maximum facet depth ranged from 99.6 to 222.7 µm. Significant differences were observed among the resin luting cements and between dual-cure and chemical-cure conditions. However, no significant differences were found between curing conditions within the universal resin luting cements. Additionally, no significant differences were identified between the hand-mixed and auto-mixed versions of the same or similar materials. CLINICAL SIGNIFICANCE: Wear resistance was strongly material dependent, but universal resin luting cements showed no influence of curing mode. A universal resin luting cement with good wear resistance may be a good option when restorative margins are difficult to illuminate.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Efficacy of light-cured luting systems for CAD-CAM milled resin indirect restorations.Revista cientifica odontologica (Universidad Cientifica del Sur) · 2026
- Repair bond strength of composite resin to additively manufactured permanent resin materials: a comparative evaluation of light-cure, self-cure, and dual-cure universal adhesivesBMC Oral Health · 2025
- Core Buildup Composite Resins Bond Strength to Dentin and Microhardness Using Universal Adhesives.Journal of functional biomaterials · 2026
- Comparative evaluation of sorption and solubility of contemporary light-cured resin cement, resin-modified glass ionomer, and self-adhesive resin luting cement in distilled water and artificial salivaJournal of Stomatology · 2026
- Comparative assessment of the resin-dentin interface using three different universal adhesives: An ex vivo studyJournal of Conservative Dentistry and Endodontics · 2026
- Interfacial Bond Strength of CAD/CAM Resin Composites on Dentin vs. Composite Substrates: Influence of Dual-Cure and Self-Adhesive Resin CementsPolymers · 2026