Efficacy of light-cured luting systems for CAD-CAM milled resin indirect restorations.
Janeth Sagrario Quintanilla-Jiménez, Jorge Alonso Borda-Bizaga, Eliam Cielo Zúñiga-Mayhua, María Soledad Peñaherrera Manosalvas, Cristian Fernando Sánchez-Puetate, Wilfredo Gustavo Escalante-Otárola
Faculty of Health Sciences, Graduate Program in Dentistry, Universidad de los Hemisferios. Quito, Ecuador. janethquintanillajimenez@gmail.com , mspenaherreram@uhemisferios.edu.ec, cfsanchezp@uhemisferios.edu.ec Universidad de Los Hemisferios Faculty of Health Sciences Graduate Program in Dentistry Universidad de los Hemisferios Quito Ecuador janethquintanillajimenez@gmail.com mspenaherreram@uhemisferios.edu.ec cfsanchezp@uhemisferios.edu.ec. · School of Dentistry, Universidad Católica de Santa María. Arequipa, Peru. jorgebordab@outlook.com, eliam.cielo@gmail.com Universidad Católica de Santa María School of Dentistry Universidad Católica de Santa María Arequipa Peru jorgebordab@outlook.com eliam.cielo@gmail.com.
Key points
From the paper's conclusion- The light-cured luting systems RelyX Veneer and Allcem Veneer APS provided superior bond strength to CAD-CAM milled resin compared with Variolink Esthetic LC, supporting their clinical use in indirect adhesive restorations.
Abstract
OBJECTIVE: To evaluate the bond strength of three light-cured luting systems for CAD-CAM milled resin indirect restorations using a shear bond strength test. MATERIALS AND METHODS: Thirty Brava Block resin cylinders were fabricated using a CAD-CAM milling unit and subjected to surface treatment with 50-μm aluminum oxide airborne-particle abrasion, ultrasonic cleaning, and application of Monobond N silane primer. Specimens were randomly assigned to three groups (Variolink Esthetic LC, RelyX Veneer, and Allcem Veneer APS) and luted according to each manufacturer's instructions. After light activation, samples were stored at 37°C for 24 hours. Shear bond strength testing was performed, and failure modes were classified. Data were analyzed using ANOVA and Tukey's post hoc test (α = 0.05). RESULTS: RelyX Veneer and Allcem Veneer APS protocols produced the highest bond strength values to CAD-CAM milled Brava Block resin (p < 0.05), with no significant difference between them (p > 0.05). Variolink Esthetic LC showed significantly lower values (p < 0.05). Cohesive failure within the milled resin predominated across all groups, while Variolink Esthetic LC exhibited a more balanced failure distribution (30% adhesive, 40% cohesive in resin, 30% mixed). CONCLUSIONS: The light-cured luting systems RelyX Veneer and Allcem Veneer APS provided superior bond strength to CAD-CAM milled resin compared with Variolink Esthetic LC, supporting their clinical use in indirect adhesive restorations.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Wear resistance of self-adhesive and universal resin luting cements.American journal of dentistry · 2026
- Interfacial Bond Strength of CAD/CAM Resin Composites on Dentin vs. Composite Substrates: Influence of Dual-Cure and Self-Adhesive Resin CementsPolymers · 2026
- Evaluation of the Integrity of Ceramic Laminates After Adhesive Cementation.Journal of esthetic and restorative dentistry : official publication of the American Academy of Esthetic Dentistry ... [et al.] · 2026
- In vitro comparison of resin cement bond strength to milled and 3D-printed resins.Journal of the mechanical behavior of biomedical materials · 2026
- Repair bond strength of composite resin to additively manufactured permanent resin materials: a comparative evaluation of light-cure, self-cure, and dual-cure universal adhesivesBMC Oral Health · 2025
- Short-term clinical performance of CAD/CAM hybrid composite and conventional indirect composite onlays in posterior teeth: A retrospective cohort study.Journal of clinical and experimental dentistry · 2026