Effects of dipping time on color parameters, elemental composition and resin cement bonding of monolithic zirconia.
Burcu Kanat-Ertürk, Cansu Akarsu, Gökçe Zengin, Funda Gül Koç, Rıdvan Yamanoğlu
Department of Prosthodontics, Faculty of Dentistry, Kocaeli University, Kocaeli, Turkey. · Department of Metallurgical and Materials Engineering, Faculty of Engineering, Kocaeli University, Kocaeli, Turkey.
Key points
From the paper's conclusion- Different dipping times significantly affected both color parameters and resin cement bond strength of monolithic zirconia. A 5-minute dipping protocol provided a favorable balance between color change and shear bond strength to resin cement.
Abstract
PURPOSE: This study evaluated the effects of different dipping times on the color parameters, elemental composition, and resin cement bonding of monolithic zirconia. MATERIALS AND METHODS: Uncolored monolithic zirconia blocks (InCoris TZI) were sectioned into 6 × 6 × 2 mm specimens (N = 44) and divided by dipping time in a coloring solution (InCoris TZI Coloring Liquids): control (C), 2 minutes (D-2), 5 minutes (D-5), and 10 minutes (D-10)(n = 10). Color measurements were performed using a dental spectrophotometer, and color differences (ΔE00) were computed using the CIEDE2000 formula. For shear bond (SBS) testing, specimens were embedded, air-abraded, primed, and bonded to resin cement cylinders (diameter: 2 mm, height: 2 mm). SBS testing was performed (0.5 mm/min.). Data were statistically assayed (SPSS 26; One-way ANOVA, Tukey post-hoc tests; P = .05). Failure modes were classified under an optical microscope. Elemental and structural analyses were performed using SEM-EDS and XRD. RESULTS: Prolonged dipping time influenced color parameters, resulting in increased ΔE00, a*, and b* values, and decreased L* values. A significant difference in ΔE00 was found between D-2 and D-10 groups(P < .05). For SBS test, D-5 group (21.76 ± 6.01 MPa) exhibited significantly higher values than C group (15.38 ± 5.77 MPa) (P < .05). SEM-EDS analysis revealed increased Er concentration and decreased Zr concentration with prolonged dipping times. Corresponding oxide-related peaks were detected by XRD. CONCLUSION: Different dipping times significantly affected both color parameters and resin cement bond strength of monolithic zirconia. A 5-minute dipping protocol provided a favorable balance between color change and shear bond strength to resin cement.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of various nanosilica coating techniques on the zirconia surface and bond strength to resin cement.Dental and medical problems · 2026
- Evaluation of the bond strength of monolithic zirconia ceramics subjected to different surface pretreatments to dental tissues.American journal of dentistry · 2026
- Color Stability of Multi-Layered Zirconia Versus Lithium Disilicate Glass Ceramic: An in Vitro Study.Journal of dental research, dental clinics, dental prospects · 2026
- Multifactorial Evaluation of Color Changes in Material Assemblies Used for Hybrid Abutment Crowns: Role of Ceramics, Surface Treatments, and Resin Cements.International journal of dentistry · 2026
- Effect of Different Surface Treatments of CAD/CAM Zirconia Core on the Final Color of Porcelain-Veneered Restorations.Journal of dental research, dental clinics, dental prospects · 2026
- Effect of Sintering Conditions and Acidic Environments on the Wear of 5Y-ZP Zirconia.Dentistry journal · 2026