Color Stability of Multi-Layered Zirconia Versus Lithium Disilicate Glass Ceramic: An in Vitro Study.
Doaa Mohamed Farahat Aboul Azm, Roqaia Mohammad Alassar, Asmaa Ahmed Mosleh, Noureldeen Mohamed Mohamed, Abdullah Waheed Faseeh, Abdelrhman Mohamed Ashour, Farag Rashed Saied
Department of Dental Biomaterials, Faculty of Dentistry, Pharos University in Alexandria, Alexandria, Egypt. · Department of Crowns and Bridges, Faculty of Dental Medicine for Girls, Al-Azhar University, Cairo, Egypt.
Key points
From the paper's conclusion- ML zirconia exhibited significantly higher color stability than LD pressable ceramic after being subjected to simulated 28 months of beverage consumption and using chlorhexidine.
Abstract
INTRODUCTION: Patients who receive ceramic restorations use daily oral care products or plaque-control agents, which may cause discoloration of these restorations. The present study assessed the color stability of multi-layered zirconia and lithium disilicate pressable ceramic after 28 days of immersion in chlorhexidine, coffee, and soda. METHODS: A disc measuring 2 mm in thickness and 10 mm in diameter was designed to fabricate 30 discs, divided into two groups based on the ceramic material: multi-layered (ML) zirconia and lithium disilicate (LD). Each group was further subdivided into three subgroups based on the staining solution: chlorhexidine, Cola, and coffee. The samples were immersed in staining liquids at room temperature for 28 days. Color was measured immediately at t0 and every week (t1, t2, t3, and t4) using a spectrophotometer. Color changes were calculated. For pairwise comparisons, the Friedman test was first employed, followed by post hoc tests. RESULTS: The greatest ∆E was observed in LD specimens immersed in chlorhexidine (5.65), followed by LD specimens immersed in coffee (5.44). The lowest ∆E was observed for ML zirconia specimens immersed in coffee (0.64). Significant differences were observed between ∆E values of all tested groups and subgroups (P≤0.05). CONCLUSION: ML zirconia exhibited significantly higher color stability than LD pressable ceramic after being subjected to simulated 28 months of beverage consumption and using chlorhexidine. CLINICAL SIGNIFICANCE: Multi-layered zirconia exhibited higher resistance to discoloration than lithium disilicate pressable ceramic. Dental professionals should inform patients about the effects of chlorhexidine, Cola, and coffee on lithium disilicate pressable restorations.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Evaluation of Color Stability and Surface Properties of Different CAD/CAM Materials: An In vitro Study.Nigerian journal of clinical practice · 2026
- Effects of Substructure Color, Cement Shade, and Aging on the Color Change of Multilayer Zirconia Laminate Veneer Restorations.Journal of functional biomaterials · 2026
- Effect of Ceramic Substrate on the Durability of Universal Stain and Glaze SystemsJournal of Esthetic and Restorative Dentistry · 2026
- Effects of Different Whitening Toothpastes on the Color of Aged Zirconia-Reinforced Lithium Silicate Ceramics After Immersion in an Acidic Beverage.BioMed research international · 2026
- Color Stability and Surface Roughness of Micro-Layered, Polished, and Glazed Zirconia Exposure to Cigarette Smoke, Tea, and Coffee.Journal of esthetic and restorative dentistry : official publication of the American Academy of Esthetic Dentistry ... [et al.] · 2026
- Influence of Khat Extract on the Color Stability of Glazed and Polished Dental Ceramics: An In Vitro Comparative Study.The journal of contemporary dental practice · 2025