Evaluation of the bond strength of monolithic zirconia ceramics subjected to different surface pretreatments to dental tissues.
Gönül M Eyüboğlu-Ateş, Ayşe Koçak-Büyükdere
Department of Prosthodontics Faculty of Dentistry, Kocaeli University, Başiskele, Kocaeli, Turkey, gmeyuboglu@gmail.com. · Department of Prosthodontics Faculty of Dentistry, Kocaeli University, Başiskele, Kocaeli, Turkey.
Key points
From the paper's conclusion- The type of dental substrate, surface pretreatment, and their interaction significantly affected SBS values (P< 0.001). Enamel groups showed higher bond strength than dentin groups (P< 0.001). The highest SBS values were obtained in the SP-E group (13.3 ± 2.3 MPa), while the lowest SBS values were obtained in the S-D group (2.5 ± 1.0 MPa).
Abstract
PURPOSE: To evaluate the laboratory bond strength of monolithic zirconia ceramics subjected to four different surface pretreatments when cemented to enamel and dentin using a dual-cure resin cement. METHODS: 120 extracted human maxillary central and lateral incisors were prepared at two levels: enamel (E) and dentin (D). Zirconia specimens (0.7 mm thick) were divided into four groups: primer (P), sandblasting + primer (SP), silane (S), and tribochemical silica + silane (TS). Each group was further divided according to the bonding substrate, resulting in eight subgroups (n=15). After surface pretreatments, specimens were cemented, subjected to thermocycling, and tested for shear bond strength (SBS). Data were statistically analyzed (P< 0.05), and failure modes were examined under a stereomicroscope. RESULTS: The type of dental substrate, surface pretreatment, and their interaction significantly affected SBS values (P< 0.001). Enamel groups showed higher bond strength than dentin groups (P< 0.001). The highest SBS values were obtained in the SP-E group (13.3 ± 2.3 MPa), while the lowest SBS values were obtained in the S-D group (2.5 ± 1.0 MPa). CLINICAL SIGNIFICANCE: This laboratory study provides some suggestions to clinicians on which surface pretreatment should be used and how deep the preparation should be during the cementation of ultra-translucent monolithic zirconia restorations. The results showed that applying an MDP-containing primer after airborne-particle abrasion and using silane following tribochemical silica coating significantly increased bond strength. In addition, keeping the preparation margins as much as possible at the enamel level enhances the long-term durability of the bond and should be prioritized in the planning of minimally invasive zirconia restorations.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of cement space, resin cement type, and surface treatment on the bond strength of monolithic zirconia copings to Ti-base abutments.The journal of advanced prosthodontics · 2026
- Evaluation of Bond Strength of Different Surface-Treated Translucent Zirconia Blocks Luted with Universal Resin Cement to Glass-Reinforced Core Composite Before and After Aging: An In vitro Study.Journal of pharmacy & bioallied sciences · 2026
- Selective Infiltration Etching as a surface modification for high-translucency zirconia: Comparative analysis of roughness, composition, and bond strength.F1000Research · 2026
- Effect of a silicon carbide bur on shear bond strength between resin cement and zirconia.Biomaterial investigations in dentistry · 2026
- Effect of Thermocycling and Surface Treatments on the Durability of Bond Strength of Translucent Zirconia to Resin Cement: An In Vitro Study.Cureus · 2026
- Shear bond strengths of primer-free and primer-based composite-cements to glass-ceramics and zirconia.Dental materials : official publication of the Academy of Dental Materials · 2026