Fracture Resistance and Failure Modes of Ultrathin Occlusal Veneers Made of Different Ceramic Materials: An In Vitro Study.
Mohamed Ezzat Elbanna, Hesham Ibrahim Othman, Ahmed Mohammed Leithy Alameldin
Fixed Prosthodontics Department, Faculty of Dentistry, Sinai University, North Sinai, Egypt. · Fixed Prosthodontics Department, Faculty of Dental Medicine, Al-Azhar University, Cairo, Egypt.
Key points
From the paper's conclusion- All the tested ceramic materials used as ultrathin occlusal veneers exhibited fracture loads significantly higher than the average physiological masticatory forces. Compared with the other two groups, LDS had the highest fracture resistance value. ZIR occlusal veneers exhibited more repairable fractures than LDS and ZLS.
Abstract
INTRODUCTION: The current in vitro study was designed to assess the failure mode and fracture resistance of ultrathin occlusal veneers made from different ceramic materials. METHODS: Twenty-four ultrathin occlusal veneers were fabricated on maxillary extracted first premolar teeth. Three ceramic materials were used: lithium disilicate (LDS), zirconia-reinforced lithium disilicate (ZLS), and zirconium dioxide (ZIR). An adhesive luting agent was used to adhesively bond occlusal veneers. Each sample was subjected to thermocycling, ranging from 5 to 55°C. Fracture resistance was tested using a universal testing machine, and fractured surfaces were examined with a stereomicroscope and a scanning electron microscope (SEM) to assess failure modes. RESULTS: A statistically significant difference was observed; the highest mean fracture resistance was observed in LDS (1741±308.3 N), followed by ZLS (1192±89.44 N), and then ZIR (866.9±60.23 N), which had the lowest mean fracture resistance. The failure mode of the ZIR group differed significantly from those of the other groups. CONCLUSION: All the tested ceramic materials used as ultrathin occlusal veneers exhibited fracture loads significantly higher than the average physiological masticatory forces. Compared with the other two groups, LDS had the highest fracture resistance value. ZIR occlusal veneers exhibited more repairable fractures than LDS and ZLS.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Load-bearing capacities of occlusal veneers made of all-ceramic and resin composite: do the substrate and material type affect mechanical durability?BMC oral health · 2026
- Impact of different surface conditioning protocols on fracture resistance of monolithic zirconia vonlay restorations.BMC oral health · 2026
- Evaluation of the Fracture Load of Multilayer Zirconia Onlay Restorations with Different Yttria Contents After Thermomechanical Aging: An In Vitro Study.Materials (Basel, Switzerland) · 2026
- The effect of different CAD/CAM materials and thickness on the immediate load-bearing capacity of occlusal veneers.Clinical oral investigations · 2026
- Biomechanical evaluation of class II inlays: The role of restorative material, resin liner, and retentive pin-hole.Clinical oral investigations · 2026
- Fracture Resistance of Lithium Disilicate and Hybrid Ceramic Crowns with Two Finish Line Thicknesses: An In Vitro Study.The journal of contemporary dental practice · 2026