The effect of different CAD/CAM materials and thickness on the immediate load-bearing capacity of occlusal veneers.
Beyza Arslandaş Dinçtürk, Ceren Başerdem, Cemile Kedici Alp, Pekka K Vallittu, Mine Betül Üçtaşli, Sufyan Garoushi, Lippo Lassila
Department of Restorative Dentistry, Faculty of Dentistry, University of Gazi, Ankara, Turkey. beyzaarslandas@gazi.edu.tr. · Department of Restorative Dentistry, Faculty of Dentistry, University of Gazi, Ankara, Turkey.
Key points
From the paper's conclusion- Both restorative material and restoration thickness play important roles in the mechanical performance of occlusal veneers. Among the evaluated CAD/CAM materials, the experimental short fiber-reinforced composite demonstrated the highest load-bearing capacity, whereas ceramic and resin-based CAD/CAM materials showed lower values. However, the higher incidence of catastrophic failures involving both restoration and tooth structure in the SFRC CAD groups indicates that fracture load alone should not be considered the only factor for material selection. These findings suggest that ultrathin occlusal veneers may have potential for minimally invasive restorative applications; however, their long-term clinical performance and failure behavior should be further investigated before clinical recommendations can be established.
Abstract
OBJECTIVES: Minimally invasive occlusal veneers fabricated from ceramic and resin-based materials have gained increasing popularity in recent years. The aim of this study was to evaluate the effect of different CAD/CAM materials and restoration thicknesses on the immediate load-bearing capacity of occlusal veneers. MATERIALS AND METHODS: A total of 100 human mandibular molars were prepared for occlusal veneers with a 1-mm circumferential rounded chamfer finish line. A preparation height of 1.5 mm extending from the preparation margin to the occlusal plane was created. The teeth were divided into 10 groups (n = 10), and occlusal veneers were fabricated in two different thicknesses (0.6 and 1.5 mm) using four CAD/CAM block materials: lithium disilicate glass ceramic (IPS e.max), nanoceramic composite (Lava Ultimate and Cerasmart 270), hybrid ceramic (Enamic), and an experimental short fiber-reinforced composite (SFRC CAD). The tested thickness of 0.6 mm is below the minimum thickness recommended by all manufacturers. Restorations were designed using Cerec software. After adhesive cementation, all specimens were stored in water at 37 °C for 2 days, followed by quasi-static loading testing. Data were analyzed using 2-way ANOVA (´restorative material´ and ´restoration thickness`) and Tukey's post hoc test (α <0.05). RESULTS: The two-way ANOVA demonstrated significant main effects of both restorative material and restoration thickness on fracture load (p < 0.001), whereas the material-thickness interaction was not significant (p = 0.200). SFRC CAD exhibited the highest fracture load (SFRC 0.6 mm = 2560.2 ± 424.5N and SFRC 1.5 mm = 2799.0 ± 655.9N) while IPS e.max (IPS e.max 0.6 mm = 1224.2 ± 363.4N and IPS e.max 1.5 mm = 1799.9 ± 436.8N) showed the lowest. Increasing restoration thickness from 0.6 mm to 1.5 mm significantly resulted in higher fracture load regardless of the restorative material. CONCLUSION: Both restorative material and restoration thickness play important roles in the mechanical performance of occlusal veneers. Among the evaluated CAD/CAM materials, the experimental short fiber-reinforced composite demonstrated the highest load-bearing capacity, whereas ceramic and resin-based CAD/CAM materials showed lower values. However, the higher incidence of catastrophic failures involving both restoration and tooth structure in the SFRC CAD groups indicates that fracture load alone should not be considered the only factor for material selection. These findings suggest that ultrathin occlusal veneers may have potential for minimally invasive restorative applications; however, their long-term clinical performance and failure behavior should be further investigated before clinical recommendations can be established. CLINICAL RELEVANCE: Occlusal veneers with a thickness of 0.6 mm, minimum thickness recommended by manufacturers, exhibited promising immediate load-bearing capacity, supporting their potential use in minimally invasive restorative. Furthermore, the experimental short fiber-reinforced composite CAD/CAM material demonstrated superior load-bearing capacity compared with the other CAD/CAM materials evaluated in this study.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Load-bearing capacities of occlusal veneers made of all-ceramic and resin composite: do the substrate and material type affect mechanical durability?BMC oral health · 2026
- Fracture Resistance and Failure Modes of Ultrathin Occlusal Veneers Made of Different Ceramic Materials: An In Vitro Study.Journal of dental research, dental clinics, dental prospects · 2026
- Evaluation of Fracture Resistance in CAD-CAM Additively Manufactured Occlusal Veneers.Polymers · 2026
- Fracture load of interim 3-unit fixed dental prostheses fabricated using contemporary CAD-CAM polymers: An in vitro study.The Journal of prosthetic dentistry · 2026
- Fracture resistance, marginal integrity, and microleakage of indirect composite and computer-aided designed-computer-aided manufactured ceramic inlays in Class II MOD cavities: An in vitro study.Journal of conservative dentistry and endodontics · 2026
- Marginal adaptation and fracture resistance of CAD/CAM-fabricated PMMA, PEEK, and PEKK three-unit provisional fixed dental prostheses: an in vitro comparative study.Biomaterial investigations in dentistry · 2026