Impact of different surface conditioning protocols on fracture resistance of monolithic zirconia vonlay restorations.
Ahmed Mahmoud El-Zagzog, Mohamed Abd El-Rahman El-Layeh, Shaimaa Ahmed Abo El-Farag
Department of Fixed Prosthodontics, Faculty of Dentistry, Mansoura University, Mansoura, Egypt. ahmadm@mans.edu.eg. · Department of Fixed Prosthodontics, Faculty of Dentistry, Mansoura University, Mansoura, Egypt.
Key points
From the paper's conclusion- Background The purpose of this study was to evaluate and compare the influence of three different surface conditioning protocols on the fracture resistance of maxillary premolars restored with monolithic multilayer zirconia vonlay restorations fabricated from two zirconia materials.
Abstract
BACKGROUND: The purpose of this study was to evaluate and compare the influence of three different surface conditioning protocols on the fracture resistance of maxillary premolars restored with monolithic multilayer zirconia vonlay restorations fabricated from two zirconia materials. METHODS: Forty-eight maxillary premolars were prepared for zirconia vonlay restorations and allocated to two groups (n = 24) according to zirconia type: Group I (C): Cercon xt ML, and Group II (K): KATANA YML. Each group was further divided into three subgroups (n = 8) based on surface treatment: subgroup (A): airborne particle abrasion; subgroup (L): Er: YAG laser; and subgroup (E): hot chemical etching. Following cementation, all specimens were subjected to 10,000 thermocycles. Axial loading was applied using a universal testing machine. Data were analyzed using two-way ANOVA and Bonferroni's post-hoc test, with one-way ANOVA conducted for each factor. RESULTS: Two-way ANOVA demonstrated that the surface treatment had a significant effect on fracture resistance (P < 0.0001), whereas the main effect of zirconia material was not statistically significant (P = 0.229). The hot chemical etching KATANA YML subgroup recorded the highest mean values, 1476.25 (177.33) N, while the airborne particle abrasion and Cercon xt ML subgroup showed the lowest mean values, 1053.33 (172.78) N. CONCLUSION: The fracture resistance values of both zirconia materials were within the accepted range for clinical application. Hot chemical etching resulted in significantly higher fracture resistance than airborne particle abrasion and Er: YAG laser treatment, while no significant difference was found between the two zirconia materials.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fracture Resistance and Failure Modes of Ultrathin Occlusal Veneers Made of Different Ceramic Materials: An In Vitro Study.Journal of dental research, dental clinics, dental prospects · 2026
- The effect of using 40% HF treatment on the shear bond strength of the zirconia surface in comparison to conventional surface treatment methods.Journal of lasers in medical sciences · 2026
- Evaluation of the Fracture Load of Multilayer Zirconia Onlay Restorations with Different Yttria Contents After Thermomechanical Aging: An In Vitro Study.Materials (Basel, Switzerland) · 2026
- Evaluation of the effect of sandblasting and laser surface treatments on the shear bond strength of zirconia with different yttria content using resin cement.Odontology · 2026
- Influence of Tooth Surface Pretreatment Procedure on Bond Strength of Self-Adhesive Cement-An In Vitro Study.Dentistry journal · 2026
- Role of cold atmospheric plasma alone or combined with conventional surface treatments on shear bond strength of 3Y-TZP and 5YSZ ceramics bonded with composite resinBiomaterial Investigations in Dentistry · 2026