From the paper's conclusion
  • This study evaluated exposure-dependent cytotoxicity of Tera Harz TC-85 and NextDent Ortho Flex and performed an exploratory screening of selected resin-specific printing conditions for ER-selective estrogen-like responses.

Abstract

Per-layer UV exposure during 3D printing may influence polymerization and the biological response of photocurable aligner resins. This study evaluated exposure-dependent cytotoxicity of Tera Harz TC-85 and NextDent Ortho Flex and performed an exploratory screening of selected resin-specific printing conditions for ER-selective estrogen-like responses. TC-85 was printed at 2.0, 2.4, 3.0, and 4.0 s per layer, and Ortho Flex at 5.0, 6.0, 7.0, and 8.0 s per layer. The resin-specific per-layer UV exposure ranges were selected based on our previous physicochemical characterization of the same materials and printing system. Extracts were prepared according to ISO 10993-12. Cytotoxicity was assessed in human gingival fibroblasts using the MTT assay, while selected conditions (TC-85, 2.4 s; Ortho Flex, 7.0 s) were evaluated in estrogen receptor (ER)-positive MCF-7 and ER-negative MDA-MB-231 cells as an exploratory screening assay rather than a direct test of ER activation. For both resins, per-layer exposure condition, extract concentration, and their interaction significantly affected the normalized MTT response. At 50% extract concentration, normalized MTT responses ranged from 89.2% to 111.3%, whereas Ortho Flex ranged from 8.8% to 76.8%, with the 8.0 s condition being the only Ortho Flex condition above the 70% cytotoxicity threshold. Ortho Flex showed pronounced cytotoxicity in concentrated extracts, particularly at shorter exposure times, whereas TC-85 showed a less monotonic exposure-dependent pattern. In the exploratory screening, the 6.25% Ortho Flex extract produced a normalized MCF-7 MTT response of 129.1%, but this was comparable with the corresponding saline vehicle response of 137.0% and was not statistically greater than the response in ER-negative MDA-MB-231 cells. No statistically supported ER-selective response was detected for either tested resin under the specific screening conditions; however, exposure-time dependence of this response was not evaluated. Per-layer UV exposure therefore influenced the HGF-1 MTT response in a resin- and concentration-dependent manner. For dental laboratory practice, these findings support the use of resin-specific, validated printing parameters rather than transferring exposure settings between materials; deviations from manufacturer-specified processing conditions should be independently validated before clinical use.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Per-Layer UV Exposure-Dependent Cytotoxicity of 3D-Printed Aligner Resins and Estrogen-like Activity Screening — Science Skim