Evaluating chemical and surface stability of thermoformed and 3D-printed clear aligners after intraoral exposure
Fabrizio Sanna, Leila Es Sebar, Isabella Sannino, Samuele Avolese, Simone Parrini, Marco Posadino, Paola Testa, Nicola Scotti,
Politecnico di Torino · University of Turin
Key points
From the paper's conclusion- These findings are consistent with recent literature, suggesting that short-term intra-oral exposure does not affect aligner materials' chemical stability.
Abstract
INTRODUCTION: Align Technology, Inc. is a leading manufacturer of orthodontic aligners, using SmartTrackTM (LD30), a multilayer aromatic thermoplastic polyurethane/copolyester, and the vacuum thermoforming process. Recently, direct 3D printing using Tera Harz TC-85 DAC resin has also been explored for the production of aligners. Both aligner materials are exposed to physical and chemical aging in the oral cavity. This study evaluates the chemical aging of these materials after 7 and 14 days of exposure to the oral environment, using Optical Microscopy, Raman spectroscopy, X-ray fluorescence (XRF), and X-ray diffraction (XRD). MATERIALS AND METHODS: Invisalign® aligners (SmartTrackTM LD30) and 3D printed aligners (Tera Harz TC-85 DAC) were worn by 20 patients for 7 (t1) and 14 days (t2). The aligners were characterized initially (t0) using Optical Microscopy, Raman spectroscopy, XRF, and XRD. After t1 and t2, each aligner was reanalyzed at three locations: right and left first molars (p1 and p2), and central incisor (p3). The results were compared with never-worn aligners (t0, n = 3). RESULTS: Both materials showed high homogeneity across all locations (p1, p2, p3) and time points, indicating uniform performance after oral exposure. PCA analysis performed on Raman spectra revealed no significant chemical changes in the surface composition after 7-14 days of use. DISCUSSION AND CONCLUSIONS: The results demonstrated that exposure to the oral environment for up to 14 days did not significantly alter the surface chemistry of either aligner material. These findings are consistent with recent literature, suggesting that short-term intra-oral exposure does not affect aligner materials' chemical stability.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Comparison of three dental resins for 3D printing of orthodontic appliances: Comparison of leaching, biocompatibility, and thermo-mechanical properties after post-curing and agingDental Materials · 2025
- Mechanical properties of thermoformed and direct-printed aligner materials after immersion in 37 °C water: a 14-day in vitro studyScientific Reports · 2026
- Advances in clear aligner therapy: comparative evaluation of the optical properties and bacterial adhesion of 3D direct-printed and thermoformed alignersProgress in Orthodontics · 2025
- Effects of intraoral ageing on the mechanical and surface properties of clear aligner materials: A systematic review.International orthodontics · 2026
- Ageing effects on chemical, physical, mechanical, and morphological properties of clear aligners - a systematic review.Progress in orthodontics · 2026
- Effect of different lengths of post-curing UV light exposure on the mechanical properties of 3D-printed aligners: An in vitro studyJournal of Orthodontics · 2025