From the paper's conclusion- The findings indicate that heat curing significantly enhances the performance of one-part geopolymers, while fiber selection provides additional mechanical and durability improvements.
Abstract
One-part geopolymer mortars provide an alternative to cementitious materials by using dry activators and industrial by-products. This study evaluated a multi-precursor matrix containing slag, fly ash, ceramic powder, red mud, and 5% MgO, reinforced with polyvinyl alcohol (PVA), basalt, or micro-steel fibers at 0.4% and 0.8% by volume. Specimens were cured at 20 ± 2 °C or at 80 °C for 24 h and assessed for flowability, mechanical properties, ultrasonic pulse velocity (UPV), Böhme abrasion, 24 h water absorption, and sorptivity. XRD, FTIR, and SEM/EDS were used only to compare by heat-cured mixtures. The results showed that at 28-day, heat curing increased compressive strength by 39.5-71.8%, flexural strength by 29.2-134.4%, and UPV by 20.5-36.4%, while reducing sorptivity by 12.2-35.7% relative to ambient curing. PVA reduced flowability likely because of its hydrophilic surface and high surface area. For 0.8PVA, the flow diameter was 23.6% below the reference, whereas the 28-day heat-cured flexural strength reached 7.5 MPa, with the lowest abrasion thickness loss of 0.63 mm. Micro-steel mixtures maintained compressive strength comparable to the reference, reaching 72-73 MPa at 28-day. Heat curing reduced water absorption in PVA and basalt mixtures, whereas the reference and micro-steel mixtures showed insignificant change. Microstructural analyses suggested the formation of a more compact and reacted aluminosilicate matrix under heat-cured conditions. A screening life-cycle assessment, limited to the non-fiber-reinforced reference matrix, showed that heat-curing increased global warming potential by 7.6%, while the two solid activators contributed approximately 45% of the ambient-cured reference GWP. The findings indicate that heat curing significantly enhances the performance of one-part geopolymers, while fiber selection provides additional mechanical and durability improvements.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of Combined Curing Regime on the Mechanical and Physical Properties of Metakaolin Based Geopolymer MortarIOP Conference Series: Earth and Environmental Science · 2026
- Mechanical and Residual Performance of Fly Ash-Based Geopolymer Mortars Incorporating Recycled Brick-Tile/Ceramic Aggregates and Polypropylene Fibers.Polymers · 2026
- Physical and microstructural characterization of wood ash–based geopolymer mortars with ceramic powder under different curing regimesConstruction and Building Materials · 2025
- Development of Alkali-Activated Phosphogypsum Mortar Incorporating Silica Fume and Metakaolin for Enhanced Durability and CO 2 MineralisationIOP Conference Series: Earth and Environmental Science · 2026
- Mechanical Properties and Microstructure of Alkali-Activated Fiber-Reinforced Mortar Incorporating Red Mud and Fly AshCrystals · 2026
- Impact of Fine Recycled Mortar Aggregates on Hydration, Microstructure, and Performance of Cementitious MaterialsApplied Sciences · 2026