IOP Conference Series: Earth and Environmental Science

Development of Alkali-Activated Phosphogypsum Mortar Incorporating Silica Fume and Metakaolin for Enhanced Durability and CO 2 Mineralisation

Joseph Gnanaraj S, Vasugi K, Govind Kumar Soni

Key points

From the paper's conclusion
  • The results demonstrate that precursor balance strongly governs the mechanical, transport, chemical and carbonation behaviour of alkali-activated PG mortar.

Abstract

This study develops an ambient-cured alkali-activated phosphogypsum (PG) mortar incorporating silica fume (SF) and metakaolin (MK) as reactive aluminosilicate precursors. Nine mixtures were produced by varying PG, SF and MK while maintaining constant total precursor, fine aggregate and alkaline activator contents. Compressive strength, water absorption, sulphate and acid resistance, porosity, accelerated carbonation and microstructural characteristics were evaluated. Among the mixtures, M3 (224 kg/m 3 PG, 504 kg/m 3 SF and 392 kg/m 3 MK) achieved the highest 28-day compressive strength of 8.60 MPa and the lowest water absorption of 0.63%. After chemical exposure, M3 retained compressive strengths of 12.23 MPa in sulphate solution and 11.19 MPa in sulphuric acid. Porosity decreased with curing age, consistent with progressive reaction and matrix densification. Accelerated carbonation produced greater CO 2 penetration than ambient curing, while carbonate formation indicated partial CO 2 mineralisation. SEM, XRD and FTIR results showed a denser reaction matrix and stronger gel-related features for M3 than M8. The results demonstrate that precursor balance strongly governs the mechanical, transport, chemical and carbonation behaviour of alkali-activated PG mortar.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Development of Alkali-Activated Phosphogypsum Mortar Incorporating Silica Fume and Metakaolin for Enhanced Durability and CO 2 Mineralisation — Science Skim