Impact of Fine Recycled Mortar Aggregates on Hydration, Microstructure, and Performance of Cementitious Materials
Renata Boris, Liudmyla Rishko, Remigijus Šalna, Yahor Trambitski, Aigerim Tolegenova
Key points
From the paper's conclusion- Overall, FRMA replacement levels of 10–20% provided the most favorable balance between recycled-material utilization and mortar performance in the investigated mixture design.
Abstract
Fine recycled mortar aggregate (FRMA) is a promising secondary raw material for cementitious composites. However, its residual porosity, high fines content, and increased water demand can adversely affect hydration and engineering performance. This study investigated the influence of FRMA through two complementary experimental series. First, Portland cement–FRMA systems containing 0–100 wt.% FRMA were evaluated by calorimetry to characterize early-age heat evolution. Second, natural sand was replaced with 10–50 wt.% FRMA in polymer- and superplasticizer-modified mortars. The mortars were assessed in terms of flowability, density, ultrasonic pulse velocity (UPV), compressive and flexural strength, and characterized by scanning electron microscopy (SEM) and X-ray diffraction (XRD). Increasing the FRMA content progressively delayed the main hydration peak and reduced cumulative heat release. The second heat-flow maximum shifted from 13.0 h for the reference paste to 17.1 h at 50% replacement, while the 48 h relative cumulative heat index decreased to 71.9%. Mortar flowability decreased by up to 12%, from 125 to 110 mm. Moderate FRMA replacement levels of 10–20% preserved density and UPV and maintained or slightly improved compressive strength. The highest 28-day compressive strength, 62.9 MPa, was obtained at 20% FRMA, approximately 3.9% above the reference value. At 30–50% replacement, density, UPV, and compressive strength decreased as the effects of porous residual mortar, higher water demand, and a higher water-to-cement ratio (W/C) became more pronounced. SEM observations confirmed greater microstructural heterogeneity at higher FRMA contents, whereas XRD showed broadly similar crystalline hydration products in all mortars. Overall, FRMA replacement levels of 10–20% provided the most favorable balance between recycled-material utilization and mortar performance in the investigated mixture design.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Fiber-Reinforced One-Part Geopolymer Mortars Incorporating Red Mud, Ceramic Powder, and MgO: Performance Under Different Curing Regimes and Curing-Based Environmental Assessment.Polymers · 2026
- Effect of Various Recycled Construction and Demolition Fines on Cementitious Mortars Rheological and Mechanical Performance.Materials (Basel, Switzerland) · 2026
- Post-Heating Performance of Concrete Containing Grading-Controlled Recycled Refractory Brick Fine AggregateConstruction Materials · 2026
- Targeted separation of adhered mortar for high-quality recycled aggregate recycling based on salt-frost separation technology: the role of sustained ice pressureCement and Concrete Composites · 2026
- Effects of Different Pretreatment Methods for Recycled Fine Aggregates on the Properties of Geopolymer Mortar Incorporating Recycled PowderBuildings · 2026
- Interface improvement and multiscale assessment of recycled concrete aggregates with epoxy resin polymerScientific Reports · 2026