Enhancing Durability and Resistance to Wear and Corrosion of AISI 431 Martensitic Stainless Steel for Sustainable Engineering Applications
Minerva Rivas-Cabanas, Carolina Camba-Fabal, José Luis Mier-Buenhombre, Laura Castro-Santos, Manuel Ángel Graña-López, Almudena Filgueira-Vizoso, Ana Isabel García-Diez
Key points
From the paper's conclusion- This study investigates the influence of heat treatment on the wear resistance and corrosion behavior of AISI 431 martensitic stainless steel, with the aim of enhancing durability and extending service life in demanding applications, thereby supporting more resource-efficient material use.
Abstract
This study investigates the influence of heat treatment on the wear resistance and corrosion behavior of AISI 431 martensitic stainless steel, with the aim of enhancing durability and extending service life in demanding applications, thereby supporting more resource-efficient material use. Two single austenitizing treatments (1000 °C and 1070 °C) and one double austenitizing treatment were evaluated. The evolution of hardness, microstructure, wear resistance, and corrosion behavior was determined as a function of the applied heat treatment. Hardness was measured using the Rockwell C method, wear behavior was evaluated by Pin-on-Disk testing, and corrosion resistance was assessed by anodic potentiodynamic polarization tests. The untreated (as-received condition) steel exhibited the lowest wear mass loss. Among the heat-treated samples, the double austenitized condition exhibited the best wear performance. The highest hardness was obtained after single austenitization at 1070 °C (approximately 50 HRC), while double austenitization and single austenitization at 1000 °C resulted in hardness values of approximately 45 HRC. Corrosion testing revealed open-circuit potentials of −0.25 V, −0.27 V, −0.13 V, and −0.14 V for the untreated, SA1000, SA1070, and double-austenitized conditions, respectively. The results show that while SA1070 and DA exhibit more noble open-circuit potentials and extend the stability window against abrupt localized collapse, the DA condition operates under a high-rate non-passive regime with an elevated current density (1.38 mA/cm2). This thermal treatment shifts the degradation mechanism away from localized intergranular vulnerability at the expense of a higher continuous dissolution rate. Consequently, while DA provides favorable wear behavior among the heat-treated conditions, its elevated current density must be carefully considered for applications in marine environments.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Assessment of Dry Sliding Wear Behavior of Annealed AISI 431 Martensitic Stainless Steel MaterialJournal of Physics: Conference Series · 2026
- Effect of thermal induction cycling on wear and corrosion performance of a X90CrMoV18 (440B) martensitic stainless steelMaterials Testing · 2026
- Effect of Tempering Temperature on the Wear Resistance of 9Cr18MoV Martensitic Bearing Steelsteel research international · 2026
- Microstructure, Wear Resistance and Corrosion Resistance of FeNiCrMo, FeNiCrMo/WC and FeNiCrMo/WC-17Co Coatings Prepared by Laser Cladding: A Comparative StudyCrystals · 2026
- Effects of PWHT on mechanical properties and corrosion resistance of dissimilar welded Optim700MC and Hardox450 steelsMaterials Testing · 2026
- Influence of Heat Treatment on Microstructure and Tribological Behavior of Conventional Maraging Steel W720 WMRJournal of Manufacturing and Materials Processing · 2026