Microstructure, Wear Resistance and Corrosion Resistance of FeNiCrMo, FeNiCrMo/WC and FeNiCrMo/WC-17Co Coatings Prepared by Laser Cladding: A Comparative Study
Jie Jiang, Zulei Liang, Jianhua Sun, Gang Li, Yuanyuan Xu, Hai Gu, Bin Li, Guoqing Dai,
Key points
From the paper's conclusion- Its specific wear rate was the lowest of the three coatings, 0.73 × 10−6 mm3·N−1·m−1 at 90 N and roughly an order of magnitude below the unreinforced coating, and its mass loss was the smallest at every load, while its corrosion resistance fell far less than that of FeNiCrMo/WC-17Co, with an Ecorr of −0.393 V against −0.738 V.
Abstract
FeNiCrMo austenitic stainless steel has good corrosion resistance but a low surface hardness, which limits its wear resistance under high load. FeNiCrMo, FeNiCrMo with 10 wt.% tungsten carbide (WC) (45–106 μm) and FeNiCrMo with 10 wt.% WC-17Co (15–45 μm) were deposited by laser cladding at 1200 W and 480 mm/min, and their phase composition, microstructure, microhardness, wear behaviour and corrosion resistance were compared. Both particle additions promoted a columnar-to-equiaxed transition and the formation of W2C. The coarse WC particles dissolved only partially and raised the hardness little, from 473 to 475 HV0.2, while the finer WC-17Co particles dissolved more completely and raised it to 550–600 HV0.2. On the worn surfaces, the ploughing grooves of the unreinforced coating were still present but shallower and narrower, indicating that abrasion was reduced in severity rather than replaced. The particles nevertheless impaired the corrosion resistance, most strongly for WC-17Co. FeNiCrMo/WC gave the best overall result. Its specific wear rate was the lowest of the three coatings, 0.73 × 10−6 mm3·N−1·m−1 at 90 N and roughly an order of magnitude below the unreinforced coating, and its mass loss was the smallest at every load, while its corrosion resistance fell far less than that of FeNiCrMo/WC-17Co, with an Ecorr of −0.393 V against −0.738 V. The coarse, only partly dissolved WC particles provide the most favourable combination of wear and corrosion resistance and are recommended for FeNiCrMo components operating under high load in only mildly aggressive conditions.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructural evolution and mechanical performance correlation of WC-reinforced iron-based coatings fabricated by laser claddingScientific Reports · 2026
- Microstructure and Wear Performance of Ni-Based Laser Cladded Coatings Reinforced with Different ZrC Contents on Structural SteelCoatings · 2026
- Effect of microstructure on corrosion and wear behavior of laser-clad CoCrFeMo0.85Ni compositionally complex alloy coatingsMaterials Today Communications · 2026
- Enhanced of friction and wear properties for TiC/TC4 coating based on the precipitation of the lubricating and strengthening phases through laser cladding of Cr–WS2–Ni60 powderJournal of Materials Research and Technology · 2025
- Influence of Laser Power on the Microstructure, Wear Resistance, and Cavitation-Erosion Behavior of Laser-Clad Fe45Cr25Ni20Ti5Mo5 Multi-Principal-Element Alloy Coatings.Materials (Basel, Switzerland) · 2026
- Effect of Laser Power on the Microstructure and Wear and Corrosion Resistance of Ni25 Alloy CoatingsLubricants · 2025