steel research international

Effect of Tempering Temperature on the Wear Resistance of 9Cr18MoV Martensitic Bearing Steel

Xiangxin Wang, Yahua Hao, Xingfu Yu, Yong Su, Yinghua Wei, Jingui Xie, Yanbin Li, Bo Li,

Key points

From the paper's conclusion
  • The results show that as the tempering temperature increased from 160 to 200 °C, the retained austenite content decreased monotonically from 22.01% to 15.35%, while the volume fraction of carbides increased monotonically from 1.23% to 2.92%.

Abstract

As a martensitic stainless steel, 9Cr18MoV steel is widely used in special bearing applications owing to its excellent wear and corrosion resistance. The effects of tempering temperature on the microstructure and mechanical properties of 9Cr18MoV steel were analyzed using optical microscopy (OM), Vickers hardness testing, X‐ray diffraction (XRD), scanning electron microscopy (SEM), and reciprocating friction and wear testing. The results show that as the tempering temperature increased from 160 to 200 °C, the retained austenite content decreased monotonically from 22.01% to 15.35%, while the volume fraction of carbides increased monotonically from 1.23% to 2.92%. This microstructural evolution led to a monotonic reduction in the hardness of the material from 711.22 HV 0.3 to 631.62 HV 0.3 . However, the wear resistance first decreased and then increased, which was related to the combined effects of hardness and microstructure, particularly the reinforcement of the carbide skeleton. The optimal wear resistance was achieved at the tempering temperature of 160 °C.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Effect of Tempering Temperature on the Wear Resistance of 9Cr18MoV Martensitic Bearing Steel — Science Skim