  • These results indicate that similar geometric section losses can be accompanied by substantially different axial deformation responses, underscoring the importance of considering both charring and applied load when evaluating GLT columns subjected to prolonged standard fire exposure.

Abstract

The fire response of large-section glued-laminated timber (GLT) columns depends on both progressive charring and sustained axial loading. This study investigated Korean larch GLT columns with a 500 mm × 500 mm cross section and a height of 3000 mm under four-sided standard fire exposure. Five non-load-bearing specimens were tested for 60–180 min, while load-bearing tests were conducted for 180 min at prescribed load ratios of 0.8, 1.0, and 1.2; the last case was excluded from quantitative comparison because its target load was not maintained. Mean charring depth increased from 39.9 mm at 60 min to 102.6 mm at 180 min, while the corresponding time-averaged charring rate decreased from 0.67 to 0.57 mm/min. A linear regression of mean charring depth against exposure duration yielded R2 = 0.993 over the 60–180 min range. After 180 min, mean charring depths were 106.5 and 107.3 mm at load ratios of 0.8 and 1.0, respectively, whereas final axial displacements were −0.66 and 18.35 mm. The equivalent residual cross-sectional area ratios calculated from the measured mean charring depths were 32.9% and 32.6%, respectively. These results indicate that similar geometric section losses can be accompanied by substantially different axial deformation responses, underscoring the importance of considering both charring and applied load when evaluating GLT columns subjected to prolonged standard fire exposure.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Experimental Investigation of Charring and Axial Deformation of Korean Larch Glued-Laminated Timber Columns Under Long-Duration Standard Fire Exposure — Science Skim