Influence of Intumescent Coating Thickness on the Thermal Response of HEA-Profile Steel Columns Under Standard Fire Exposure
Adrian Simion, Andreea Hegyi, Daniela-Mihaiela Boca, Claudiu-Sorin Dragomir, Tudor Panfil Toader
Key points
From the paper's conclusion- This study investigates how intumescent coating thickness affects the thermal response of six HEA 300 specimens made of S235 steel.
Abstract
Fire protection of structural steel is essential for limiting heating and preserving load-bearing capacity under fire exposure. This study investigates how intumescent coating thickness affects the thermal response of six HEA 300 specimens made of S235 steel. Measured mean dry film thickness (DFT) ranged from 1.01 to 1.88 mm. Specimens were exposed on four sides to the nominal ISO 834 standard fire curve, without applied mechanical loading and their time to reach selected steel-temperature thresholds was compared. At an adopted reference temperature of 550 °C (assumed utilization factor μ0 = 0.6160), the times reported in the experimental dataset ranged from 32 to 36 min. Specimens S4, S2, and S3 (DFT of 1.34, 1.60, and 1.88 mm) each reached 550 °C after 36 min, whereas specimen S6 (1.78 mm) reached it after 34 min. These results indicate a non-monotonic relationship between mean coating thickness and thermal response under the investigated conditions. Post-exposure observations showed local detachment of the coating, although its occurrence during the test was not determined. The reported times provide comparative thermal-performance indicators, not a standalone standardized load-bearing fire-resistance classification.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Predicting Performance of Intumescent Coatings Using Medium‐Scale TestingFire and Materials · 2026
- Enhancing fire resistance in steel structures through innovative coating materialsWorld Journal of Advanced Research and Reviews · 2026
- Experimental Investigation of Charring and Axial Deformation of Korean Larch Glued-Laminated Timber Columns Under Long-Duration Standard Fire ExposureMaterials · 2026
- Post‐Fire Mechanics of Corroded Q690 High‐Strength Steel and Influence on H‐Shaped ColumnsMaterials and Corrosion · 2026
- Recent Advances in Modification Strategies for Intumescent Fire-Protective Coatings for Steel StructuresCoatings · 2026
- Hot-Dip Galvanized Steel in Fire: Linking NIR/MIR Reflection to Early-Stage Heating Delay Under Standard Fire ExposureCoatings · 2026