Mix-Proportion Design and Properties of Steel Slag-Based Composite Cementitious Materials Using a Constrained Four-Component Mixture Design.
Qiaoming Guo, Yuanbao Liu, Hui Chen, Zhengbin Luo, Bin Liu, Minghui Lin, Liu Yang, Zuming Chen,
Jiangxi Provincial Communications Investment Group Co., Ltd., Nanchang 330108, China. · Jiangxi JPCI Maintenance Technology Group Co., Ltd., Nanchang 330108, China.
Key points
From the paper's conclusion- This study investigated a four-component system comprising steel slag (SS), blast furnace slag (BFS), ordinary Portland cement (OPC), and desulfurized gypsum (DG), using 17 formulations within a constrained four-component mixture design.
Abstract
High-volume utilization of steel slag in cementitious materials requires a proportioning method that accounts for coupled effects among multiple components. This study investigated a four-component system comprising steel slag (SS), blast furnace slag (BFS), ordinary Portland cement (OPC), and desulfurized gypsum (DG), using 17 formulations within a constrained four-component mixture design. Unlike previous studies focused mainly on ternary binders or empirical proportioning, this work combined four-component formulation screening with age-dependent hydration characterization in one SS-BFS-OPC-DG framework. The 7 d compressive strength was selected as the modeled response because it provided a consistent early-age basis for comparing all 17 formulations within a practical testing period, whereas flexural strength was retained as a complementary experimental response. The compressive-strength mixture model was significant (p = 0.0044), with R2 = 0.692, adjusted R2 = 0.589, predicted R2 = 0.435, and adequate precision = 8.545. Its performance was evaluated using prediction indices, residual diagnostics, and an independent confirmation batch. The selected mass fractions of SS, BFS, OPC, and DG were 0.322, 0.429, 0.131, and 0.116, respectively. The confirmation batch achieved a 7 d compressive strength of 24.80 MPa, compared with the predicted value of 24.93 MPa. The model was therefore used only for formulation screening and interpolation within the investigated component ranges. The selected formulation reached compressive and flexural strengths of 32.6 and 7.6 MPa at 28 d, respectively. XRD, SEM, TG, and FTIR results collectively supported continued formation of hydration products and progressive matrix densification from 3 d to 28 d. The C-S-H gel index increased from 2.07% to 6.15%, while the number of large visible voids decreased and the continuity of the matrix improved. These results provide a constrained mixture-design route for screening high-solid-waste SS-BFS-OPC-DG binders.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of high-content steel slag on granulated blast furnace slag–desulfurized gypsum-based cementitious materials: Long-term volume stability and hydration mechanismsResults in Engineering · 2025
- PERFORMANCE EVALUATION OF SLAG MODIFIED CONCRETE USING MACHINE LEARNING TECHNIQUESKufa Journal of Engineering · 2026
- Impact of high-volume steel slag with varying particle sizes on engineering properties of micro silica- modified concreteDiscover Materials · 2026
- Mechanical and Durability Properties of Concrete Using Sugarcane Bagasse Ash and Steel SlagAdvances in Civil Engineering · 2026
- Synergistic Effect of Ground Granulated Slag, Steel Slag, and Carbonation Treatment on the Strength and Microstructure of Ultra‐High‐Performance Slag ConcreteAdvances in Civil Engineering · 2026
- Steel Slag and Iron Ore Tailings in Cementitious Mine Backfill: Material Functions, Gel Evolution, and Engineering SelectionGels · 2026