Impact of high-volume steel slag with varying particle sizes on engineering properties of micro silica- modified concrete
Bengin M. A. Herki, Nasser Firouzi
Key points
From the paper's conclusion- The results show the engineering potential of moderate SS replacement and MS incorporation as well as the need for direct microstructural, expansion and life cycle evaluation in the future.
Abstract
The use of steel slag (SS) as partial replacement of natural fine and coarse aggregates and micro silica (MS) as partial replacement of cement was experimented with respect to engineering performance of concrete. In the present study, 0–70% of the natural sand and gravel, respectively, were replaced by fine steel slag (FSS) and coarse steel slag (CSS) as replacements on an absolute-volume basis. Also 10% MS was added to selected mixes in which 0%, 30%, 50%, and 70% SS was used. Workability, density, compressive strength, splitting tensile strength, flexural strength, sorptivity, ultrasonic pulse velocity (UPV) and performance in an adopted modified freeze–thaw exposure protocol were assessed. The SS-only mixtures showed the best compressive strength of 42.1 MPa which was obtained from the 40% SS mixture with no MS. However, when the SS replacement level increased, the compressive strength values decreased, even though the density of the concrete was increased, for example, to 70% SS, compressive strength was reduced to 31.8 MPa. The tested combinations of mixtures containing MS had 30% SS + 10% MS with the best overall combination of mechanical and durability related properties measured. The improvements observed herein are similar to those reported in literature for the filler and pozzolanic effects but were not directly ascertained in the present study by microstructural characterization, and thus specific changes in the interfacial transition zone, pore structure or C–S–H formation are not directly obtained. Likewise, the occurrence of possible volumetric instability and microcracking at high SS replacement levels are literature-supported interpretations, due to the absence of measurement of free CaO/free MgO contents and expansion. The results of the freeze-thaw test, based on the modified exposure protocol, are comparative in nature and do not represent standard performance. The results of a screening-level embodiment of carbon comparison showed that the 30% SS + 10% MS mixture has the highest calculated compressive-strength-to-embodied-carbon ratio of all the mixtures tested. The results show the engineering potential of moderate SS replacement and MS incorporation as well as the need for direct microstructural, expansion and life cycle evaluation in the future.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Experimental Study on Rheological, Mechanical Properties and Microstructure of Ultra-High Performance Concrete (UHPC) Mixed with Steel Slag PowderMaterials · 2026
- Mechanical and Durability Properties of Concrete Using Sugarcane Bagasse Ash and Steel SlagAdvances in Civil Engineering · 2026
- Microscopic and Macroscopic Performance Analysis of Steel Slag-modified Roller-Compacted Concrete: Implications in the Development of Sustainable InfrastructureIOP Conference Series: Earth and Environmental Science · 2026
- Effect of steel slag as fine aggregate on the mechanical and durability performance of concrete under acid exposureScientific Reports · 2025
- PERFORMANCE EVALUATION OF SLAG MODIFIED CONCRETE USING MACHINE LEARNING TECHNIQUESKufa Journal of Engineering · 2026
- Effect of high-content steel slag on granulated blast furnace slag–desulfurized gypsum-based cementitious materials: Long-term volume stability and hydration mechanismsResults in Engineering · 2025