Synergistic Effect of Ground Granulated Slag, Steel Slag, and Carbonation Treatment on the Strength and Microstructure of Ultra‐High‐Performance Slag Concrete
Sana T. Abdulhussain, Maan S. Hassan, Shatha S. Hasan
Key points
From the paper's conclusion- Eighteen mixtures and three parameters, including 20%–60% GGBFS, 25%–75% steel slag, and 25%–75% carbonation level, were designed using the central composite design (CCD) to investigate their complementary role in improving the microstructure and strength of ultra‐high‐performance slag concrete (UHPSC).
Abstract
The production of ultra‐high‐performance concrete (UHPC) requires large amounts of cement (up to 1000 kg/m 3 ), quartz powder, and silica sand, thereby imposing an environmental burden and depleting natural resources. This study investigates the integration of CO 2 into slag cement by continuously immersing particle surfaces in a saturated CO 2 environment to produce sustainable binders. This work focuses on the subsequent value‐added use of captured CO 2 to enhance the binding properties of alkali‐activated slag. The synergistic effect of CO 2 curing with the incorporation of ground granulated blast‐furnace slag (GGBFS) as a cement replacement and carbonated inert steel slag as a replacement for quartz sand was evaluated. Eighteen mixtures and three parameters, including 20%–60% GGBFS, 25%–75% steel slag, and 25%–75% carbonation level, were designed using the central composite design (CCD) to investigate their complementary role in improving the microstructure and strength of ultra‐high‐performance slag concrete (UHPSC). Second‐order polynomial models and numerical optimization were performed to correlate the investigated parameters and the targeted responses accurately. Response surface analysis reveals that GGBFS and carbonation are the key drivers of the behavior of 28‐day compressive and flexural strength. The results demonstrated that the 28‐day compressive and flexural tensile strengths reached 178.07 and 35.13 MPa, respectively. The statistical validation and model checking confirmed high model reliability ( R 2 of 89% for compressive strength and 97% for flexural strength). Fourier transform infrared (FTIR), X‐ray diffraction (XRD), and scanning electron microscopy (SEM) analyses show that CO 2 pre‐treatment of slag particles effectively produced calcite and silica gel, stabilizing and densifying the hydrate phases.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Utilisation and activation strategies of steel slag for ultra-high-performance concrete: A comprehensive reviewJournal of Building Engineering · 2026
- Cost-effective and sustainable ultra-high-performance concrete with electric arc furnace slag and calcium carbonate: a multi-objective optimization and experimental validation approachScientific Reports · 2026
- Carbon sequestration mechanisms and performance evolution of alkali-activated slag during the mixing processMaterials Science-Poland · 2026
- Mechanical and Durability Properties of Concrete Using Sugarcane Bagasse Ash and Steel SlagAdvances in Civil Engineering · 2026
- Sustainable design of high strength ECC using steel slag as fine aggregate: Toward waste valorization and environmental benefitsSustainable Chemistry and Pharmacy · 2025
- Evaluation and prediction of self-healing performance of ultra-high-performance concrete based on the entropy weight method and response surface methodologyENGINEERING Structure and Civil Engineering · 2026