Resource Utilization of Limestone Powder and Steel Slag Powder in Cement-Based Materials at Extremely Low Water/Binder Ratio.
Yuchen Han, Yuchen Li, Hongyi Zhang, Qihan Liu, Fanghui Han
Department of Civil Engineering, School of Future Cities, University of Science and Technology Beijing, Beijing 100083, China.
Key points
From the paper's conclusion- The results show that limestone powder promotes the early strength development of concrete at an extremely low w/b ratio better than steel slag powder does under standard curing conditions, but steel slag powder promotes the late strength growth better.
Abstract
The large-scale resource utilization of limestone powder generated from mining operations and steel slag waste discharged from the metallurgical industry is of vital importance. The effects of limestone powder or steel slag powder on the properties of cement-based materials at an extremely low water/binder (w/b) ratio of 0.16 under standard curing and early high-temperature curing at 60 °C for 3 d were comparatively studied through measuring the compressive strength, hydration degree and microstructure. The results show that limestone powder promotes the early strength development of concrete at an extremely low w/b ratio better than steel slag powder does under standard curing conditions, but steel slag powder promotes the late strength growth better. For concrete containing 10% and 20% steel slag powder, the compressive strength increased by 20.4 and 33.7 MPa, respectively, from 3 to 7 d, and the difference in their compressive strengths was only 0.4 MPa at 90 d. The limestone powder promotes strength more significantly under early high-temperature curing conditions; however, when the dosage reaches 30%, the long-term strength of the concrete containing steel slag powder is marginally greater compared to the concrete containing limestone powder. At 90 d under early high-temperature curing, the chemically bound water contents of the pastes containing limestone powder ranged from 9.05% to 10.53%, compared with 10.64% to 11.85% for the pastes containing steel slag powder. The diffraction peak intensity of ettringite is stronger in the paste with limestone powder due to the stabilizing effect of limestone powder on ettringite. The diffraction peak intensity of Ca(OH)2 is stronger in the paste with steel slag powder, which exhibits a higher hydration degree and generates more hydration products. The pore structure of the sample containing steel slag powder improves, and the microstructure becomes denser at high temperatures.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Experimental Study on Rheological, Mechanical Properties and Microstructure of Ultra-High Performance Concrete (UHPC) Mixed with Steel Slag PowderMaterials · 2026
- Compressive Strength and Microstructure of All-Solid-Waste Concretes Modified with Basalt Fiber or Biochar: A Comparative Study of Carbide Slag-Based and Steel Slag-Based SystemsBuildings · 2026
- Carbon utilization for low-carbon concrete: Prospects for carbonated steel slag and recycled concreteResources Conservation and Recycling · 2025
- Mechanical and Durability Properties of Concrete Using Sugarcane Bagasse Ash and Steel SlagAdvances in Civil Engineering · 2026
- Enabling the High-Volume Utilization of Iron-Rich Sewage Sludge Ash in Cement: The Role of Curing Temperature in Microstructure and Performance Enhancement.ACS omega · 2026
- Impact of high-volume steel slag with varying particle sizes on engineering properties of micro silica- modified concreteDiscover Materials · 2026