Enabling the High-Volume Utilization of Iron-Rich Sewage Sludge Ash in Cement: The Role of Curing Temperature in Microstructure and Performance Enhancement.
Kao Chen, Yaxin Xiao, Shuang Liu, Yi Ren, Weiwei Zhu
School of Materials and Environment, Guangxi Key Laboratory of Advanced Structural Materials and Carbon Neutralization, Guangxi Engineering Research Center for Advanced Materials and Intelligent Manufacturing, Guangxi Minzu University, Nanning 530105, China.
Key points
From the paper's conclusion- These findings elucidate the regulatory role of curing temperature in the hydration and microstructural evolution of high-volume SSA ternary blends, providing theoretical guidance for curing regime optimization in engineering practice.
Abstract
The massive generation of sewage sludge ash (SSA) poses severe environmental challenges worldwide. Ternary blended cement incorporating SSA and limestone represents a promising green cementitious material that enables high-volume SSA utilization, yet the retarding effect of SSA on cement hydration leads to unsatisfactory early compressive strength, which remains the primary bottleneck restricting its large-scale engineering application, particularly at high replacement levels. In this work, the compressive strength development, hydration heat evolution, phase assemblage, and pore structure of SSA-limestone-cement blends cured at 5 °C, 20 °C, and 40 °C were systematically investigated to reveal the temperature-dependent hydration mechanism. The results show that elevated curing temperature accelerates early hydration and improves the 3-day compressive strength, while curing at 20 °C yields the highest late-age strength. Based on hydration calorimetry, X-ray diffraction (XRD), thermogravimetric analysis, and mercury intrusion porosimetry (MIP), the underlying micro-mechanism is clarified: curing at 5 °C results in the lowest 3-day and 28-day strength due to sluggish hydration reactions and abundant harmful macropores. At 20 °C, the 3-day strength is slightly lower than that at 40 °C owing to the delayed hydration acceleration period, but the substantial formation of ettringite (AFt) and carboaluminate phases at later ages refines the pore structure and gives rise to the maximum 28-day compressive strength. Curing at 40 °C achieves the highest early strength via accelerated hydration, yet the transformation of AFt to AFm and the accumulation of portlandite (CH) generate an unfavorable pore structure and limit late-age strength growth. These findings elucidate the regulatory role of curing temperature in the hydration and microstructural evolution of high-volume SSA ternary blends, providing theoretical guidance for curing regime optimization in engineering practice. This work offers a feasible pathway to promote the high-value utilization of iron-rich SSA in cementitious materials and contributes to carbon reduction in the cement industry.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of sewage sludge ashes on the performance of cementitious compositesMaterialia · 2026
- A low-carbon supplementary cementitious material via synergistic utilization of coal gangue and calcium carbide slag for sulphoaluminate cementConstruction and Building Materials · 2025
- Sewage sludge ash in concrete: a comprehensive review on properties, performance, and environmental sustainabilityDiscover Civil Engineering · 2026
- Low-carbon cementitious grouts with straw biochar and ladle furnace slag: A micro- to macro-scale investigationConstruction and Building Materials · 2026
- Calcium Chloride Activation of Acid-Washed Sewage Sludge Ash: Hydration Mechanism and Performance as a Supplementary Cementitious Material.Molecules (Basel, Switzerland) · 2026
- Hydration, mechanical, and environmental performance of blended cements incorporating ground granulated blast furnace slag, ground waste bottle glass, and metakaolinFrontiers in Materials · 2026