Influence of Ni Contents and Local Hydrogen Concentration on Crack Propagation in FCC Fe-Ni Alloy Models: A Molecular Dynamics Study.
Kaimeng Wang, Yingli Li, Molin Su, Hongqiao Yan, Yue Zhao, Lei Zhao
CNPC Research Institute of Safety & Environment Technology, Beijing 102206, China. · School of Materials Science and Engineering, Tianjin University, Tianjin 300350, China.
Key points
From the paper's conclusion- The results show that local hydrogen introduction has a limited effect on the peak stress-strain response, while hydrogen clearly accelerates crack propagation in the middle stage, especially at high concentrations.
Abstract
This study investigates the atomic-scale effects of hydrogen concentration and Ni content on crack propagation in Fe-Ni alloy models using molecular dynamics methods. A Mode I crack model with a (001)[100] orientation was constructed, and hydrogen atoms were locally introduced at the crack tip with concentrations of 5.3 at.% and 14.3 at.%. Fe-Ni alloy models with 5%, 10%, 15%, and 20% Ni were compared in terms of crack growth, dislocation evolution, stacking fault energy, and hydrogen diffusion. The results show that local hydrogen introduction has a limited effect on the peak stress-strain response, while hydrogen clearly accelerates crack propagation in the middle stage, especially at high concentrations. For the 10% Ni model, the middle-stage crack growth rate increases to 0.36 Å/ps under 14.3 at.% crack-tip hydrogen. Crack growth in all models shows three stages. The 15% Ni model exhibits a clear plateau in the second stage and the shortest final crack length. Further analysis shows that Ni content regulates dislocation behavior through stacking fault energy. At 15% Ni, sustained dislocation entanglement and high-density dislocation multiplication occur near the crack tip, which helps dissipate local stress. Hydrogen diffusion analysis indicates that hydrogen mobility is lower in the 15% Ni model, which may be related to hydrogen retention near dislocation-rich regions. A normalized comparison based on hydrogen diffusion and middle-stage crack growth rate further identifies 15% Ni as the lowest crack propagation tendency composition among the studied models. These results provide atomic-scale data for Ni-content optimization in hydrogen-resistant alloys, although the direct engineering transfer of the findings is limited by the length and time scales of molecular dynamics simulations.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Atomistic Insights into Hydrogen Diffusion and Deformation Mechanisms in FeCrNi-Based Austenitic Stainless Steels: Effects of Alloying, Temperature, and Hydrogen ConcentrationMolecules · 2026
- The effects of hydrogen on the mechanical properties of CoCrFeMnNi high-entropy alloy: Molecular dynamics simulationJournal of Applied Physics · 2026
- Atomic-Scale Insights into Hydrogen-Induced Ductile-to-Brittle Transition in Polycrystalline α-Fe with Varying Hydrogen Concentrations and Grain Sizes.Materials (Basel, Switzerland) · 2026
- Atomistic insights into hydrogen-assisted fracture in a polycrystalline Al matrix model for 7075 aluminum alloyModelling and Simulation in Materials Science and Engineering · 2026
- Hydrogen-assisted fatigue crack growth of pipeline steels under gaseous hydrogen pressure: A unified anisotropic phase-field modelEuropean Journal of Mechanics - A/Solids · 2026
- Experimental and molecular dynamics evaluation of grain size effects on hydrogen trapping and mechanical performance of pipeline steelJournal of Materials Science: Metallurgy · 2026