Atomic-Scale Insights into Hydrogen-Induced Ductile-to-Brittle Transition in Polycrystalline α-Fe with Varying Hydrogen Concentrations and Grain Sizes.
Peifen Yao, Yaoyinqi Wang, Qiaosheng Zhang, Shengde Di, Xiaoming Luo
College of Pipeline Engineering, Xi'an Shiyou University, Xi'an 710065, China. · Research Institute of Petroleum Engineering Technology, SINOPEC Shanghai Offshore Oil & Gas Company, Shanghai 200120, China.
Key points
From the paper's conclusion- The results demonstrate that, with increasing hydrogen concentration, hydrogen atoms preferentially diffuse along grain boundaries and gradually reach segregation saturation, resulting in continuous degradation of mechanical properties.
Abstract
With the development of hydrogen pipelines, hydrogen embrittlement has become a critical issue affecting the safe service of pipeline steels. However, the critical hydrogen concentration for the hydrogen-induced ductile-to-brittle transition and its dependence on grain size remain unclear. Molecular dynamics simulations were performed to elucidate the effects of hydrogen concentration and grain size on the hydrogen-induced ductile-to-brittle transition by investigating hydrogen diffusion, dislocation emission, and fracture evolution in polycrystalline α-Fe. The results demonstrate that, with increasing hydrogen concentration, hydrogen atoms preferentially diffuse along grain boundaries and gradually reach segregation saturation, resulting in continuous degradation of mechanical properties. The initial fracture strain of both fine-grained and coarse-grained models decreases by more than 40%, while fracture energy decreases by more than 50%. Crack surface areas increase by factors of 2.48 and 1.86, respectively, indicating greater hydrogen sensitivity of the fine-grained model. At grain-boundary hydrogen concentrations of approximately 7-9%, suppressed grain-boundary dislocation emission triggers the transition from plastic deformation to brittle intergranular fracture, marking the onset of the hydrogen-induced ductile-to-brittle transition. A quantitative relationship between grain size and grain-boundary atom fraction was established to predict the critical hydrogen concentration for this transition. This study reveals the role of hydrogen concentration in regulating dislocation emission and intergranular fracture, providing insights for hydrogen embrittlement assessment and pipeline material design.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Experimental and molecular dynamics evaluation of grain size effects on hydrogen trapping and mechanical performance of pipeline steelJournal of Materials Science: Metallurgy · 2026
- Atomistic insights into hydrogen-assisted fracture in a polycrystalline Al matrix model for 7075 aluminum alloyModelling and Simulation in Materials Science and Engineering · 2026
- Influence of grain boundary energy on hydrogen segregation tendenciesComputational Materials Science · 2026
- Machine learning interatomic potential reveals hydrogen embrittlement origins at general grain boundaries in α-ironCommunications Materials · 2025
- A hydrogen-informed Rice-Beltz model for crack-tip dislocation emission under mixed-mode loadingarXiv · 2026
- The effects of hydrogen on the mechanical properties of CoCrFeMnNi high-entropy alloy: Molecular dynamics simulationJournal of Applied Physics · 2026