Experimental and molecular dynamics evaluation of grain size effects on hydrogen trapping and mechanical performance of pipeline steel.
Meekness Nnoka, Omar Faye, Tonye Alaso Jack, Jerzy Szpunar
Department of Mechanical Engineering, University of Saskatchewan, 57 Campus Drive, Saskatoon, Saskatchewan S7N 5A9 Canada.
Key points
From the paper's conclusion- The results showed that finer-grained steels exhibited higher apparent hydrogen solubility, indicating longer hydrogen residence times in the steel with higher grain boundary density, while coarser-grained steels had higher hydrogen diffusivity.
Abstract
This study investigated the effect of grain size on hydrogen trapping and the mechanical performance of steels before and after hydrogen ingress. Using annealing treatments, different average grain sizes of 8, 11.5, 13, and 19 μm were obtained. Hydrogen permeation and slow strain rate tensile (SSRT) tests were conducted in air and hydrogen environments. The results showed that finer-grained steels exhibited higher apparent hydrogen solubility, indicating longer hydrogen residence times in the steel with higher grain boundary density, while coarser-grained steels had higher hydrogen diffusivity. Under in-situ hydrogen charging, all samples showed a slight increase in yield strength and reduced ductility; however, fine-grained samples exhibited significantly greater ductility loss and earlier failure. Fractography confirmed more quasi-cleavage features in the fine-grained steels. Additionally, molecular dynamics simulations supported these findings, revealing a significant reduction in ductility in finer-grained samples, confirming a greater susceptibility to hydrogen embrittlement.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Atomic-Scale Insights into Hydrogen-Induced Ductile-to-Brittle Transition in Polycrystalline α-Fe with Varying Hydrogen Concentrations and Grain Sizes.Materials (Basel, Switzerland) · 2026
- The role of pearlite lamellae spacing on hydrogen permeationInternational Journal of Hydrogen Energy · 2026
- Effects of prior austenite grain size on hydrogen embrittlement behavior in high-strength martensitic steelMaterials Science and Engineering A · 2025
- Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part II: Some Aspects of the Microstructural Mechanisms of Hydrogen-Assisted Damage and FractureMetals · 2026
- Atomistic insights into hydrogen-assisted fracture in a polycrystalline Al matrix model for 7075 aluminum alloyModelling and Simulation in Materials Science and Engineering · 2026
- Investigation of Welded Joints of Pipelines from an Existing Gas Transmission Network Exposed to Hydrogen—Part I: Structure, Mechanical Properties and Susceptibility to Hydrogen EmbrittlementMetals · 2026