Surface Durability and Mechanical Performance of Sustainable KOH-Activated Hybrid Fly Ash Mortars for Flooring Layers.
Robinson Rúa-Patiño, Edison A Hincapie-Atehortua, Sergio A Arboleda-Lopez, Andres F Urrego-Higuita, M A Rico, Ary A Hoyos-Montilla
Faculty of Architecture and Engineering, Institución Universitaria Colegio Mayor de Antioquia, Medellin 050035, Colombia. · Faculty of Architecture, Universidad Nacional de Colombia, Medellin 050034, Colombia.
Key points
From the paper's conclusion- The results showed that OPC exhibited the highest strength and lowest wear; among the hybrid mortars, 90/10-8 M exhibited the highest relative performance, while 80/20-8 M provided the best balance between cement reduction, strength, and wear.
Abstract
Sustainable mortars for flooring require mechanical stability and surface durability against abrasion, not only compressive strength. This study evaluates potassium hydroxide (KOH)-activated hybrid fly ash mortars as candidate materials for sustainable flooring and surface wear layers. Ordinary Portland cement (OPC) was partially replaced with fly ash (FA) at OPC/FA ratios of 90/10, 80/20, and 70/30, using 4 M and 8 M KOH solutions. The experimental program included the characterization of fly ash, the alkaline solution, and fine aggregate, as well as flowability, bulk density, compressive strength, abrasion mass loss, and numerical consistency analysis. The results showed that OPC exhibited the highest strength and lowest wear; among the hybrid mortars, 90/10-8 M exhibited the highest relative performance, while 80/20-8 M provided the best balance between cement reduction, strength, and wear. The integrated mechanical-surface performance index IMS and the analytical-numerical consistency assessment enabled the formulations to be ranked using an integrated selection criterion.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Residual Mechanical Performance and Mass Loss of Heat-Cured NaOH-Activated Fly Ash/Slag and Portland Cement Mortars After Exposure to Elevated TemperaturesBuildings · 2026
- Synergistic Impact of Bio-Based and Waste-Derived Contents on the Mechanical and Thermal Performance of Alkali-Activated Slag Mortars.Polymers · 2026
- Mechanical and durability performance of sustainable cement mortars: Experimental optimization and multi-regression modellingNext Materials · 2026
- Effect of Fly Ash Mechanical Activation on the Rheology, Hydration, Strength, and Microstructure of Cementitious SystemsInfrastructures · 2026
- Mechanical and Microstructural Performance of Mortars with Ladle Furnace Slag after Thermal ExposureJournal of Physics: Conference Series · 2026
- Fiber-Reinforced One-Part Geopolymer Mortars Incorporating Red Mud, Ceramic Powder, and MgO: Performance Under Different Curing Regimes and Curing-Based Environmental Assessment.Polymers · 2026