Mechanical and Microstructural Performance of Mortars with Ladle Furnace Slag after Thermal Exposure
Tayná Fracão da Silva, Everton de Freitas Cordova de Souza, Eduardo Freire Mariano, Gisleiva Cristina dos Santos Ferreira, Armando Lopes Moreno Junior, Josiane
Key points
From the paper's conclusion- The results indicated that the LFS+MK combination exhibited the best performance among the mixtures at elevated temperatures, with greater preservation of the residual mechanical properties after thermal exposure.
Abstract
To mitigate the environmental liabilities generated by the steel and construction industries, several studies have investigated the use of solid waste as a supplementary cementitious material. Among these materials, ladle furnace slag (LFS) stands out due to its chemical and mineralogical characteristics, including its high CaO content and the presence of other oxides such as Fe 2 O 3 and Al 2 O 3 . In this context, the production of blended mortars with the replacement of hydrated lime (HL) by LFS is included, a use that still requires more in-depth studies, for example, regarding its performance under fire situations. Therefore, this research aims to determine the residual mechanical properties of blended mortars with total replacement of HL by LFS, as well as partial replacement (10%) of Portland cement by metakaolin (MK). To this end, the mortars were subjected to elevated temperatures. The experimental stage included casting prismatic specimens (40 mm × 40 mm × 160 mm) and maintaining them under laboratory conditions for 90 days. Subsequently, they were subjected to temperatures of 200 °C, 400 °C, and 600 °C at a heating rate of 4 °C/min, with procedures adapted from RILEM TC 200-HTC:2007, Part 2. After the specimens were cooled inside the furnace at the same rate used during heating, flexural strength, compressive strength, dynamic modulus of elasticity, and scanning electron microscopy tests were performed. Specimens kept at room temperature served as reference data. The results indicated that the LFS+MK combination exhibited the best performance among the mixtures at elevated temperatures, with greater preservation of the residual mechanical properties after thermal exposure. This behavior may be associated with the combined effects of cementitious reactions and the filler effect of LFS, contributing to a denser matrix and improved resistance to thermally induced damage.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Residual Mechanical Performance and Mass Loss of Heat-Cured NaOH-Activated Fly Ash/Slag and Portland Cement Mortars After Exposure to Elevated TemperaturesBuildings · 2026
- The effect of the cooling process of ferrochrome slag waste on its performance as a sustainable supplementary cementitious material.Environmental science and pollution research international · 2026
- Mechanical and Thermal Behavior of Mortars Containing Waste Foundry Sand Exposed to High TemperaturesJournal of Physics: Conference Series · 2026
- Multiscale Evaluation of the High-Temperature Performance of Cement Mortars Containing Class C and F Fly Ash.Materials (Basel, Switzerland) · 2026
- Residual performance of Portland cement types-based plain and steel fibre-reinforced mortars exposed to elevated temperaturesResults in Engineering · 2025
- Mechanical and Residual Performance of Fly Ash-Based Geopolymer Mortars Incorporating Recycled Brick-Tile/Ceramic Aggregates and Polypropylene Fibers.Polymers · 2026