Materials (Basel, Switzerland)

Effect of ER:YAG Laser Irradiation on the Load-Bearing Capacity and Reliability of All-Ceramic Zirconia Crowns.

Natália Piffer Pasquali, Patrícia Moreira de Freitas, Márcia Borba, Paula Benetti

Post-Graduation Program in Dentistry, University of Passo Fundo (UPF), Passo Fundo 99052-900, RS, Brazil. · Special Laboratory of Lasers in Dentistry (LELO), School of Dentistry-USP, São Paulo 05508-000, SP, Brazil.

Key points

From the paper's conclusion
  • Er:YAG laser irradiation of the cementation surface did not affect the load-bearing capacity or structural reliability of zirconia crowns.

Abstract

BACKGROUND: This study evaluated the effect of Erbium:Yttrium-Aluminum-Garnet (Er:YAG) laser irradiation on the fracture load, failure mode, and reliability of monolithic and porcelain-veneered zirconia crowns. METHODS: Monolithic ultra-translucent zirconia crowns (5YZ-M, n = 30) and porcelain-veneered zirconia crowns (3YZ-V, n = 30) were divided into control (Ctrl-no surface treatment) and Er:YAG laser irradiation (Las) groups (n = 15). Las was performed on the cementation surface (250 mJ, 10 Hz, 2.5 W for 30 s). Crowns were adhesively cemented onto dentin-analog abutments and subjected to compressive load-to-failure testing. Data were analyzed by two-way ANOVA, Tukey's post hoc test, and Weibull analysis (α = 0.05). Fractographic analysis was performed. RESULTS: Laser irradiation did not affect the fracture load (p = 0.183). Monolithic crowns (5YZ-M) showed significantly higher fracture load than veneered crowns (3YZ-V) (p < 0.001). There was no effect of the interaction between factors (p = 0.150). The m-values were similar among groups, while the L0 of 3YZ-V-Ctrl was significantly lower than that of 5YZ-M. Veneered restorations predominantly showed chipping and delamination; whereas, monolithic crowns mainly exhibited catastrophic failures. Fracture origins were mostly located at the occlusal loading area. CONCLUSIONS: Er:YAG laser irradiation of the cementation surface did not affect the load-bearing capacity or structural reliability of zirconia crowns.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers

Effect of ER:YAG Laser Irradiation on the Load-Bearing Capacity and Reliability of All-Ceramic Zirconia Crowns — Science Skim