Microstructure and Mechanical Properties of Laser-MIG Hybrid Welding of Invar36 Alloy with Different Grooves
Dehao Kong, Shiwei Zhang, Hong Bian, Jun Tao, Dong Yang, Xiaoguo Song, Caiwang Tan
Commercial Aircraft Corporation of China (China) · Harbin Institute of Technology
Key points
From the paper's conclusion- The results indicated that the grain growth morphologies and grain sizes varied among the grooves.
Abstract
Laser-MIG hybrid welding experiments were performed on 10 mm thick Invar36 alloy plates. The influence of three different types of welding grooves (V-shape, rectangle, and X-shape) on the microstructure and mechanical properties of the welded joints were analyzed. The results indicated that the grain growth morphologies and grain sizes varied among the grooves. The average grain size at the center of the weld seam was 177.97 μm, which was smaller than the top grain size of 317.29 μm and the bottom grain size of 233.59 μm. In V-shape and rectangle grooves, the dimensions of grain the first weld pass was obviously smaller than the top region of the second pass. Microstructural characterization and tensile test showed no vertically columnar grains along the weld centerline in rectangle grooves which significantly affected the mechanical properties of welded joints. As a result of this phenomenon, V-shape groove joints demonstrated better mechanical properties than rectangle groove joints. The highest average tensile strength for V-shape groove, X-shape groove, and rectangle groove joints were 429.0 MPa, 419.3 MPa, and 395.4 MPa, respectively. Based on the Abaqus software, three-dimensional finite element analyses of three groove types were performed to investigate the relationship between microstructure and groove geometries. It was observed that the higher KAM regions in the EBSD results correlated with the higher effective plastic deformation in the finite element analysis. Furthermore, it was inferred from the thermal cycle curves that variations in thermal cycles across different regions resulted differences in grain size and grain growth morphology.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Microstructural evolution and strengthening mechanisms of gas tungsten arc welded nickel-based superalloy joints processed by laser powder bed fusion: Effects of welding direction and heat inputJournal of Materials Processing Technology · 2025
- Mechanical Integrity of Inconel 617-AISI 304H Steel-Welded Joints Fabricated by Pulsed GTAWMetallurgical and Materials Transactions A · 2025
- Continuous and pulsed TIG welded joint of ASTM A105-AISI 316L steels: Characterization of microstructure, mechanical properties, and fracture analysisJournal of Materials Research and Technology · 2025
- Microstructural Evolution and Mechanical Properties of AA2017 Aluminum Alloy Joints Produced by Rotary Friction Welding and TIG Welding.Materials (Basel, Switzerland) · 2026
- Microstructural, mechanical and corrosion properties of handheld laser-welded Inconel 625 joints: a comparison between autogenous welding and ERNiCrMo-3 filler wire additionMaterials Testing · 2026
- Research on the influence of segmented surface pretreatment of rolls on the interfacial bonding and crack inhibition of Ni60A repair layer by laser claddingJournal of Materials Research and Technology · 2025