Microstructural Evolution and Mechanical Properties of AA2017 Aluminum Alloy Joints Produced by Rotary Friction Welding and TIG Welding.
Piotr Noga, Anna Kula, Marcel Wiewióra, Tomasz Skrzekut
Faculty of Non-Ferrous Metals, AGH University of Krakow, Mickiewicza 30 Av., 30-059 Krakow, Poland.
Key points
From the paper's conclusion- The results demonstrate that the joint formation mechanism is the primary factor governing the microstructural evolution and mechanical performance of AA2017 alloy joints.
Abstract
This study investigates the influence of joining technology on the microstructural evolution and mechanical properties of joints produced from extruded AA2017 aluminum alloy rods. Rotary Friction Welding (RFW) was compared with conventional TIG welding to evaluate the effects of solid-state and fusion-based joining mechanisms. The joints were characterized using scanning electron microscopy (SEM), energy-dispersive spectroscopy (EDS), electron backscatter diffraction (EBSD), hardness measurements, tensile testing, and fracture analysis. TIG welding produced a coarse-grained cast microstructure within the fusion zone, whereas RFW generated a fine-grained microstructure formed through intense thermomechanical deformation accompanied by crystallographic texture evolution. These distinct microstructural characteristics resulted in markedly different mechanical behavior. The RFW joints achieved an ultimate tensile strength of 247 MPa and an elongation to failure of 12.5%, compared with 160 MPa and 1.7%, respectively, for the TIG-welded joints. The results demonstrate that the joint formation mechanism is the primary factor governing the microstructural evolution and mechanical performance of AA2017 alloy joints.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Investigation of tensile properties and microstructure in dissimilar AA2219–AA2014 friction stir welded aluminium alloysMaterials Today Communications · 2026
- Synergistic effects of PWHT and FSP on the microstructure, texture and mechanical properties of tungsten inert gas–welded dissimilar AA7075-T6/AA6061-T6 jointsMaterials Today Communications · 2026
- Friction stir welding of dissimilar metals: Investigating the role of interlayers in aluminium-steel butt joint performanceMaterials Today Communications · 2025
- Effects of the Ratio of Rotation to Welding Speed on the Mechanical Properties of the Friction-Stir Welds of the Dissimilar Aluminum Alloys AA5052-H32 and AA6261-T6Applied Sciences · 2026
- Mechanical and electrochemical analysis of AA5083-AA7075 dissimilar alloy joints fabricated by friction stir weldingDiscover Materials · 2026
- Recent progress and perspectives in fusion welding of Mg-RE alloys: From weldability fundamentals to process-microstructure correlationJournal of Magnesium and Alloys · 2025