Microstructural, mechanical and corrosion properties of handheld laser-welded Inconel 625 joints: a comparison between autogenous welding and ERNiCrMo-3 filler wire addition
Hasan Atik, Mustafa Tümer, Ş. Hakan Atapek, Alptekin Kısasöz, Tolga Mert
Kocaeli Üniversitesi · Yıldız Technical University
Abstract
Abstract This study investigates the microstructural, mechanical, and corrosion properties of Inconel 625 alloy joints produced by fiber laser welding, both autogenously and with ERNiCrMo-3 filler metal. Macrostructural analysis confirmed defect-free welds with increased weld metal volume in filler-added joints. Autogenous welding yielded finer grain structure, but higher concentrations of brittle Laves phase precipitates, leading to increased hardness yet reduced ductility and early crack initiation. Conversely, filler metal welds exhibited coarser grains, lower Laves phase formation, and superior tensile strength and elongation. Corrosion testing revealed the base material possessed the highest corrosion resistance, while filler metal welds demonstrated increased corrosion rates attributed to grain coarsening. These findings highlight the critical influence of welding metallurgy on joint performance, indicating that filler metal use enhances mechanical properties at a moderate compromise in corrosion resistance, guiding optimal welding strategies for Inconel 625 applications.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Investigating the Effects of Iron Dilution on the Corrosion Resistance of Inconel 625 Welding Overlay on Carbon SteelMaterials · 2025
- Weldability assessment, microstructural evolution, and mechanical performance of Hastelloy X weld metals using different filler metals via GTAWJournal of Materials Research and Technology · 2026
- Microstructure, Corrosion Resistance and Mechanical Properties of Dissimilar Welded Austenitic, Super-Austenitic and Duplex Stainless Steels.Materials (Basel, Switzerland) · 2026
- Effect of Ni-based filler metal types on microstructure and cryogenic impact toughness of FCAW welded 9 % nickel steelJournal of Materials Research and Technology · 2025
- Microstructure and corrosion resistance of friction stir welded 6061 aluminum alloy joints中国焊接:英文版 · 2026
- Mechanical Integrity of Inconel 617-AISI 304H Steel-Welded Joints Fabricated by Pulsed GTAWMetallurgical and Materials Transactions A · 2025