Heat-Treatment-Induced Phase Evolution in DED-Fabricated Ti-11Nb-9Fe Alloy and Its Impact on the Microstructure–Hardness Relationship
Dimakatso Moyan, Wallace R. Matizamhuka, Khathutshelo M. Nemavhola, Kabelo M. Raselabe, Nana K. Arthur, Mikateko F. Baloyi
Key points
From the paper's conclusion- This study examines how solution treatment and aging affect the phase evolution, microstructure and local mechanical properties of a DED-fabricated Ti-11Nb-9Fe metastable β-titanium alloy.
Abstract
Directed energy deposition (DED) offers a flexible route for producing near-net-shape titanium components. However, its rapid thermal cycles can cause chemical heterogeneity and microstructural features that affect mechanical performance. This study examines how solution treatment and aging affect the phase evolution, microstructure and local mechanical properties of a DED-fabricated Ti-11Nb-9Fe metastable β-titanium alloy. The alloy was deposited from elemental Ti, Nb and Fe powders using an Optomec 850-R LENS system. It was then solution-treated at 1100 °C for 24 h, water-quenched, and aged at 500 and 600 °C for 4, 8 and 12 h. The as-printed and heat-treated alloy was characterised by OM, SEM, EDS, XRD, EBSD, Vickers microhardness and nanoindentation. The as-printed alloy was heterogeneous, consisting of fine equiaxed β grains with ≈18% α in partly dissolved, Ti-rich particle regions. Solution treatment removed this heterogeneity and produced coarse, equiaxed, single-phase β (≈99.9%). Aging precipitated α within the retained β matrix without changing the β-grain structure, and no TiFe was detected. At 500 °C, the α was fine and uniformly distributed. At 600 °C, it first nucleated at grain boundaries and then developed into coarser acicular laths. As a result, hardness increased steadily during aging at 500 °C, reaching 493 ± 22 HV0.5 after 12 h, ≈31% above the solution-treated condition. Aging at 600 °C gave only modest hardening, which peaked after 8 h and decreased slightly with prolonged holding as the α coarsened. Nanoindentation confirmed these trends and showed that aging raised the indentation modulus from 102 to 128–143 GPa. These results provide a basis for choosing heat treatments for DED Ti-11Nb-9Fe: 500 °C/12 h gives the highest hardness, while the solution-treated condition offers the lowest modulus.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effect of heat treatment on microstructure and hardness of DED-fabricated Ti-11Nb-9Fe alloyMATEC Web of Conferences · 2026
- Comparative evaluation of phase constitution and microstructure in directed energy deposition additively manufactured CP-Ti, Ti-11Nb and Ti-9Fe alloysMATEC Web of Conferences · 2026
- Evolution of the Metallographic Structure of Additively Manufactured Ti-6Al-4V and Ti-6Al-7Nb Titanium AlloysMaterials · 2025
- Tailoring the Mechanical Properties of L‐DED‐Fabricated γ‐TiAl Alloys Through Heat Treatment: Correlating Microstructural Evolution With Fracture MechanismsRare Metals · 2026
- Simulation framework and thermal descriptor extraction for directed energy deposition of Ti-Nb-Zr alloysMATEC Web of Conferences · 2026
- Tensile deformation behavior of Ti-Nb graded alloy fabricated by direct laser depositionAdvanced Light Materials · 2026