Comparative evaluation of phase constitution and microstructure in directed energy deposition additively manufactured CP-Ti, Ti-11Nb and Ti-9Fe alloys

Mavis Khathusthelo Nemavhola, Wallace R. Matizamhuka, Nana K.K. Arthu, Ronald Machaka

Key points

From the paper's conclusion
  • These findings indicate that Fe, with a Mo-equivalent approximately seven times higher than Nb per weight percent, more effectively suppresses the β → α/α′ transformation under the rapid solidification conditions of DED, retaining a near-equal β + α/α′ dual-phase constitution compared to the predominantly martensitic Ti-11Nb microstructure.

Abstract

β-type titanium alloys are widely used for advanced structural applications due to their high strength-to-weight ratio and corrosion resistance. Alloying elements such as niobium (Nb) and iron (Fe) are commonly used as β-stabilisers; however, Nb is expensive and may pose processing challenges during additive manufacturing due to its high melting temperature. In this study, CP-Ti, Ti-11Nb and Ti-9Fe alloys were fabricated using Directed Energy Deposition Additive Manufacturing (DED-AM) and analysed using XRD, OM, SEM and EBSD. The results of Ti-9Fe displayed a nearly equal dual-phase β + α/α’ distribution, whereas Ti-11Nb displayed a primarily α/α’ microstructure with a significant ω-phase content (22.33 vol.%). The Vickers microhardness results showed that Ti-9Fe had 428±61 HV0.5 while Ti-11Nb had 258±9 HV0.5, indicating the impact of phase composition on mechanical response. These findings indicate that Fe, with a Mo-equivalent approximately seven times higher than Nb per weight percent, more effectively suppresses the β → α/α′ transformation under the rapid solidification conditions of DED, retaining a near-equal β + α/α′ dual-phase constitution compared to the predominantly martensitic Ti-11Nb microstructure.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers