MATEC Web of Conferences

Effect of heat treatment on microstructure and hardness of DED-fabricated Ti-11Nb-9Fe alloy

Dimakatso Moyan, Wallace R. Matizamhuka, Khathutshelo Nemavhola, Kabelo M. Raselabe, Nana K.K. Arthur

Key points

From the paper's conclusion
  • These results suggest that the DED-fabricated Ti-11Nb-9Fe alloy is optimally strengthened by aging at 500°C.

Abstract

Directed Energy Deposition enables the production of near-net-shape titanium parts with complex geometries. However, rapid solidification, residual stresses and chemical segregation may lead to microstructural heterogeneity. Thus, heat treatment after deposition is required to homogenise the microstructure and to control the phase evolution in metastable β-Ti alloys. The present work was aimed at producing DED Ti-11Nb-9Fe alloy and subsequently solution-treating it at 1100°C for 24 hrs, water-quenching and aging at 500°C and 600°C for 4, 8 and 12 hrs in an argon atmosphere. Effects of aging temperature and holding time on phase evolution, microstructural evolution and hardness were studied by X-ray diffraction (XRD), optical microscopy, scanning electron microscopy and Vickers microhardness measurements. Solution treatment gave a more homogeneous β-microstructure and reduced segregation. XRD analysis showed β-related reflections in the as-built condition, while additional α-related reflections became evident after aging, indicating α-phase formation within the retained β matrix. The aging heat treatment at 500°C was most effective in forming fine secondary features in the β matrix and showed the highest hardness of 493±22 HV0.5 after 12 hrs. On the other hand, at 600°C, microstructural coarsening and lower hardness values were observed, indicating the onset of over-aging. These results suggest that the DED-fabricated Ti-11Nb-9Fe alloy is optimally strengthened by aging at 500°C.

Read the paper

Discussion

Science Skim's AI key points, plus readers' public thoughts

Readers' thoughts

No reader thoughts yet.

Related papers