Repair Bond Durability of Selected Thermally Aged CAD/CAM-Milled and 3D-Printed Provisional Restorative Materials Following Different Surface Treatment Protocols: A Comparative In Vitro Study
Zeynep Irkeç, Ayben Şentürk
Key points
From the paper's conclusion- This study examined differences between a selected CAD/CAM-milled PMMA and a 3D-printed resin material, along with the effects of surface treatment and repair material on shear bond strength (SBS) and failure behavior.
Abstract
Background: Repair durability remains a concern for digitally fabricated provisional restorations. This study examined differences between a selected CAD/CAM-milled PMMA and a 3D-printed resin material, along with the effects of surface treatment and repair material on shear bond strength (SBS) and failure behavior. Methods: Forty CAD/CAM-milled PMMA and forty 3D-printed provisional resin specimens underwent 5000 thermocycles in artificial saliva before repair. Each material group comprised four subgroups (n = 10) combining untreated or air-abraded and adhesive-treated surfaces with bis-acryl or universal resin composite repairs. After repair, specimens underwent another 5000 thermocycles in artificial saliva before SBS and failure mode assessment. Analyses included three-way ANOVA, HC3 robust tests, adjusted comparisons, failure mode analysis and correlation analysis. Results: Material system (p = 0.005), surface treatment (p < 0.001), and the surface treatment × repair material interaction (p = 0.006) were significantly associated with SBS. Repair material had no statistically significant overall effect, although HC3 detected an effect in milled specimens (p = 0.0088). The highest SBS was observed in surface-treated 3D-printed specimens repaired with universal composite (35.14 ± 7.92 MPa), whereas the lowest was recorded in untreated CAD/CAM-milled specimens repaired with the same material (2.72 ± 1.32 MPa). Cohesive-type failures increased from 0% (untreated) to 57.5% (treated), reaching 100% in treated 3D-printed specimens. Conclusions: The selected 3D-printed resin exhibited higher SBS than the tested CAD/CAM-milled PMMA under the experimental conditions, without establishing a general advantage of either manufacturing method. Universal composite yielded the lowest untreated and highest treated SBS values, while neither repair material consistently outperformed the other, emphasizing the importance of substrate-specific surface treatment.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Influence of surface pretreatments on the repair bond strength of 3D-printed resin used for permanent restorations: an in vitro study.Frontiers in dental medicine · 2026
- Repair bond strength of composite resin to additively manufactured permanent resin materials: a comparative evaluation of light-cure, self-cure, and dual-cure universal adhesivesBMC Oral Health · 2025
- Chairside Repair of Provisional Restorative Materials: Effects of Material Type, Repair Protocol, and Thermocycling on Shear Bond Strength.Materials (Basel, Switzerland) · 2026
- Surface Treatment and Pre-Repair Thermal Aging Effects on Repair Bond Strength of Resin-Matrix CAD/CAM Ceramics.Biomimetics (Basel, Switzerland) · 2026
- Optimizing Interfacial Bonding of Additive Manufactured Resin via Combined Surface Treatments: An In Vitro Study on 3D-Printed Fixed Lingual Retainers.Journal of functional biomaterials · 2026
- Effect of different bonding agents and airborne-particle abrasion on shear bond strength and mode of failure between 3D-printed denture tooth-colored specimens and 3D-printed denture bases.BMC oral health · 2026