Optimizing Interfacial Bonding of Additive Manufactured Resin via Combined Surface Treatments: An In Vitro Study on 3D-Printed Fixed Lingual Retainers.
Pyi Phyo Win, I-Ying Huang, Daniel De-Shing Chen, Szu-Yu Lai, Yuichi Mine, Tong-Hsien Chow, I-Ta Lee, Chien-Fu Tseng,
School of Dentistry, College of Oral Medicine, Taipei Medical University, Taipei 110301, Taiwan. · Department of Oral Hygiene, College of Dental Medicine, Kaohsiung Medical University, Kaohsiung 807378, Taiwan.
Key points
From the paper's conclusion- These findings suggest that the combination of APA and RMPP improves resistance to in vitro hydrothermal degradation, although intraoral durability of interface-only 3DR retainers requires further clinical validation.
Abstract
Fixed lingual retainers fabricated from 3D-printed resin (3DR) offer the benefits of geometric freedom; however, conventional approaches frequently rely on encapsulation or oversized retention pads to compensate for limited adhesion, increasing bulk and undermining these advantages. This study evaluated an interface-only bonding protocol using combinations of mechanical and chemical surface treatments for 3DR. Specimens were assigned to five groups: control; airborne-particle abrasion (APA) followed by universal adhesive (UA); APA followed by resin-matrix-penetrating primer (RMPP); non-thermal handheld plasma (NTHP) followed by UA; and NTHP followed by RMPP. Surface roughness, wettability, and chemical composition were characterized using contact profilometry, water-contact angle measurements, and attenuated total reflectance Fourier-transform infrared spectroscopy, respectively. Shear bond strength (SBS) and failure modes were evaluated before and after 10,000 thermal cycles. APA-containing protocols significantly increased surface roughness, whereas NTHP-containing protocols improved wettability without detectable topographical changes. Distinct chemical signals associated with urethane dimethacrylate and 10-methacryloyloxydecyl dihydrogen phosphate were identified in the RMPP- and UA-treated groups, respectively. Pre-aging SBS was comparable among groups, whereas APA followed by RMPP produced the highest post-aging SBS, and UA-containing groups showed the lowest values. These findings suggest that the combination of APA and RMPP improves resistance to in vitro hydrothermal degradation, although intraoral durability of interface-only 3DR retainers requires further clinical validation.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Comparative effects of plasma activation and monomer infiltration on the surface characteristics and wettability of 3D-printed permanent crown resin.Journal of dental sciences · 2026
- Repair Bond Durability of Selected Thermally Aged CAD/CAM-Milled and 3D-Printed Provisional Restorative Materials Following Different Surface Treatment Protocols: A Comparative In Vitro StudyJournal of Functional Biomaterials · 2026
- Effect of different bonding agents and airborne-particle abrasion on shear bond strength and mode of failure between 3D-printed denture tooth-colored specimens and 3D-printed denture bases.BMC oral health · 2026
- Effects of Surface Pretreatment Protocols on Interfacial Gap Volume and Shear Bond Strength in the Composite Repair of a Definitive 3D-Printed Dental Resin: An In Vitro Study.Journal of functional biomaterials · 2026
- Effects of chemical surface treatment on shear bond strength between additively manufactured denture base and autopolymerizing resins in non-aged conditions.Journal of prosthodontic research · 2026
- Combined Effects of Print Orientation and Post-Curing Duration on the Mechanical and Surface Properties of a 3D-Printable Resin Intended for Lingual Retainers: An In Vitro Study.Polymers · 2026