Effect of Prolonged Self-Etching Ceramic Primer Application and Reaction Protocols on Surface Characteristics and Shear Bond Strength of CAD/CAM Ceramics: An In Vitro Study
Hessa Alotaibi, Ayman M. Sulimany, Ahmed Maawadh, Thamer Almohareb
Key points
From the paper's conclusion- Under the tested laboratory conditions, the combined 60/120 s MEP protocol produced higher SBS after thermocycling than HF+S for the two lithium disilicate-based ceramics, whereas HF+S produced the highest SBS for the feldspathic ceramic.
Abstract
This study evaluated the effects of prolonged self-etching ceramic primer protocols on surface roughness (Ra), topography, shear bond strength (SBS), and failure modes of three CAD/CAM ceramics. Lithium disilicate (IPS e.max CAD), advanced lithium disilicate (CEREC Tessera), and feldspathic ceramic (VITABLOCS Mark II) specimens received hydrofluoric acid etching plus silane (HF+S) or Monobond Etch & Prime (MEP). For MEP, active application and passive reaction times were increased together using paired durations of 20/40, 40/80, or 60/120 s, respectively (n = 10 per group). Ra was measured by optical profilometry, and additional specimens underwent qualitative scanning electron microscopy. SBS was measured after 10,000 thermocycles, followed by failure-mode classification. Ra and SBS were analyzed using two-way ANOVA and Tukey’s HSD; failure modes were analyzed using the Fisher–Freeman–Halton test. Ceramic material, treatment, and their interaction significantly affected Ra and SBS (p < 0.001). For both lithium disilicate-based ceramics, SBS did not differ significantly between MEP 40/80 s and HF+S, whereas MEP 60/120 s produced significantly higher SBS than HF+S. HF+S produced the highest SBS for feldspathic ceramic. Failure-mode distributions differed across the material–treatment groups (p < 0.001). Under the tested laboratory conditions, the combined 60/120 s MEP protocol produced higher SBS after thermocycling than HF+S for the two lithium disilicate-based ceramics, whereas HF+S produced the highest SBS for the feldspathic ceramic.
Read the paper
Discussion
Science Skim's AI key points, plus readers' public thoughts
Readers' thoughts
No reader thoughts yet.
Related papers
- Effectiveness of self-etching ceramic primer on the bond strength of lithium disilicate glass-ceramics: A systematic review and meta-analysis of in vitro studies.Journal of prosthodontic research · 2026
- Effect of Silane Spacer Length on Initial Bonding and Durability of Feldspathic CeramicsApplied Sciences · 2026
- Surface Treatment and Pre-Repair Thermal Aging Effects on Repair Bond Strength of Resin-Matrix CAD/CAM Ceramics.Biomimetics (Basel, Switzerland) · 2026
- Effect of Surface Treatments and Bonding Agents on Microshear Bond Strength of Zirconia-Reinforced Lithium Silicate and Conventional Glass-Ceramics: Silane Versus Universal Adhesive.Polymers · 2026
- Repair Bond Durability of Selected Thermally Aged CAD/CAM-Milled and 3D-Printed Provisional Restorative Materials Following Different Surface Treatment Protocols: A Comparative In Vitro StudyJournal of Functional Biomaterials · 2026
- Effect of Surface Treatment Protocols on Nanoindentation-Derived Mechanical Properties and Wettability of Hybrid CAD/CAM Materials.Dentistry journal · 2026